1) rolled sheet meta
轧制薄板
3) wide and thin plate rolling
宽薄板轧制
4) cold-rolled sheet
冷轧薄板
1.
Experimental study of recrystallization of cold-rolled sheets produced by CSP hot bands;
CSP冷轧薄板再结晶试验研究
2.
The main production process,equipments collocation and advanced technologies of the primary cold-rolled sheet project are introduced in this paper.
介绍了莱钢冷轧薄板(一期)工程的主要生产工艺、设备配置及先进技术。
3.
Newly-built cold-rolled sheet project in Jigang is introduced and the process flows, technological characteristics and the technical parameters of main facilities in 110×104 tons continuous pickling line, 84×104 tons cold rolling line, 43×104 tons annealing line, 48×104 tons leveling line and 33×104 tons recoiling and cutting line are analyzed with emphasis.
介绍了济钢新建冷轧薄板项目的情况,重点介绍了110万t连续酸洗线、84万t冷轧线、43万t退火线、48万t平整线和33万t重卷分卷线的工艺流程、技术特点及主要设备技术参数。
5) hot rolled strip
热轧薄板
1.
In this paper,the mechanisms of formation of rolled-in scale and scale mark are analyzed which are the major surface defects of continuous hot rolled strip used for cold rolling.
针对供冷轧用热轧薄板表面出现的氧化铁皮麻点表面缺陷,介绍了氧化铁皮压入与氧化铁皮麻点形成的机理,并分析了该缺陷的成因,结合首钢迁钢2160热轧线实际生产经验,提出了预防和减少该缺陷的措施。
6) Hot Rolled Sheet
热轧薄板
1.
The microscope,SEM,EDS and so on are used to analysis the reasons of the edge cracks of the hot rolled sheet.
采用化学成分分析、金相检验、扫描电镜及能谱分析等方法对连铸连轧(CSP)工艺生产的热轧薄板出现边裂的原因进行了分析。
补充资料:薄板
薄板
sheet
b0Obon薄板(sheet)厚度为0.2一4mm、以单张定尺供应的板材。生产方法主要分为热轧和冷札两类。现代热连轧机生产(见热连札宽带钢生产)的薄板最小厚度为1.Zmm。以叠轧方式热轧(见登札薄板生产)则能生产最小厚度为0.28mm的叠轧薄板。现代冷轧机生产的薄板,厚度更薄(0 .Zmm以下)且尺寸公差更为严格。 (李生智李隆旭)