说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 微波高值铁氧体谐振子系列
1)  Qmicroweve high-Q ferrite resonator series
微波高值铁氧体谐振子系列
2)  microwave YIG ferrite
YIG系微波铁氧体
3)  microwave lithium ferrite
微波锂系铁氧体
4)  ferrite resonator
铁氧体谐振器
5)  microwave ferrite
微波铁氧体
1.
According to the functional requirement and material characteristic of microwave ferrite substrates,the simulation process of relative motion trace was studied in the parallel lapping and polishing area by using coordinate transformation method,and it provided the theoretic foundation for the reasonable selection of processing parameters.
针对微波铁氧体基片的功能要求和材料特性,基于坐标变换法对平行式研磨、抛光加工区域的相对运动轨迹进行仿真研究,为合理选择工艺参数提供理论依据;通过正交化实验分析各种工艺参数对研磨效率的影响规律;在此基础上,采用优化组合的工艺参数进行微波铁氧体基片平行式研磨和抛光加工,技术指标均达到或超过了使用要求。
2.
The wide temperature stability and high power are the important properties of microwave ferrite s research all the time.
宽温度稳定性,大功率一直是微波铁氧体材料研究的重点。
3.
A novel microwave ferrite thin-film transformer based on Si IC technology was presented.
实现了一种新型的基于硅IC工艺的微波铁氧体集成薄膜变压器。
6)  resonant wave train
谐振波列
补充资料:镍-铝微波铁氧体
分子式:Ni-Al
CAS号:

性质:又称镍-铝微波铁氧体。在镍旋磁铁氧体基础上,用三价铝离子置换一部分三价铁离子形成的镍-铝旋磁铁氧体。化学式为NiAlxFe2-xO4。当Alx的x值达约0.7%,磁性出现反常现象,这时材料已无实用值。按铝含量而分为0.1≤x≤0.4和0.7≤x≤1.0两类旋磁铁氧体。饱和磁化强度0.035~0.145T,随铝量换量的增加而降低。居里温度155~440℃。铁磁共振线宽18.0~44.0kA/m(9kHz)。介电常数8.2~9.5。介质损耗角正切值(3~50)×10-4。采用电子陶瓷工艺,热压烧结或氮气氛烧结。适于制作高功率器件。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条