2) full-penetration weld
全焊透焊缝
3) fusion penetration
焊透;焊透深度
4) transmission welding
透射焊接
1.
Fixture design of laser transmission welding plastics;
激光塑料透射焊接夹具设计
2.
Experiment research on laser transmission welding of two different thermoplastics
两种不同热塑性塑料之间的激光透射焊接试验
3.
The influence of laser transmission welding parameters for polypropylene(PP) plastics on welding quality is investigated by orthogonal design method.
利用正交实验方法,研究了聚丙烯(PP)塑料的激光透射焊接工艺参数对焊接质量的影响。
5) lack of penetration
未焊透
1.
In order to improve detection precision, the method of detecting T-type fillet weld lack of penetration height was discussed using ramp probe in the wing.
为提高检测精度,探讨了用斜探头在翼板上检测T型角焊缝未焊透高度的方法。
2.
The tensile experimental results of four group L 3R welding test specimen included defect free and with above plate part,defect free and no above plate part,with lack of penetration and above plate part,with lack of penetration and no above plate part were presented in this work.
报道了L3 R焊接试板在无缺陷有焊缝余高、无缺陷无焊缝余高、有未焊透有焊缝余高、有未焊透无焊缝余高四组试样的拉伸试验结果和L3 R热轧板和焊接板的裂纹张开位移试验结果。
3.
The lack of penetration (LOP) is a very common type of discontinuities in welds,so that how to simplify it more scientifically and reasonable and therefore to conduct its fracture analysis are a problem continuously interested to engineering and academic circles.
未焊透是工程实际焊接结构中最为常见的一种焊接不连续 ,如何更科学合理地简化未焊透工程 ,以便于对其进行的断裂分析是工程界和学术界所一直关心的问题。
6) incomplete penetration
未焊透
1.
Ultrasonic detecting method of incomplete penetration depth of T-joint weld;
T型接头组合焊缝未焊透深度的超声检测方法
2.
Effects of incomplete penetration on the stress concentration of lattice frame empty spheric joint;
未焊透对网架空心球节点应力集中的影响
3.
However, the researches into the pipe tees with incomplete penetration defects are inadequate.
三通是压力管道系统中不可缺少的管道元件,但国内对存在未焊透缺陷的三通研究很少。
补充资料:未焊透
分子式:
CAS号:
性质:焊接时钝边根部未完全熔合的现象叫未焊透。未焊透使焊缝强度降低,压力容器焊缝一般不允许未焊透存在,应及时返修。
CAS号:
性质:焊接时钝边根部未完全熔合的现象叫未焊透。未焊透使焊缝强度降低,压力容器焊缝一般不允许未焊透存在,应及时返修。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条