1)  adhesive-coated catalyzed laminate
涂胶催化层压板
2)  adhesive-coated uncatalyzed laminate
涂胶无催层压板
3)  catalytic coating
催化涂层
4)  photocatalytic coating
光催化涂层
1.
TiO 2 photocatalytic coating was then prepared on a slide substrate, with ethyl silicate as the binder.
采用溶胶-凝胶法制得了添加La2O3 的改性TiO2 微粉,用硅酸乙酯作粘结剂,将TiO2 光催化涂层涂覆在载玻片上,讨论了TiO2 含量(质量分数,下同)以及活性炭和沸石对涂层光催化活性的影响。
5)  zeolite coating
涂层催化剂
1.
In this work, an investigation was conducted to explore the zeolite coating catalytic cracking of jet fuel model compound (n-dodecane) and the practice fuel (China No.
采用X射线衍射,傅立叶红外光谱仪,和扫描电子显微镜对涂层催化剂进行了表征。
6)  catalyst coating
催化剂涂层
1.
Therefore catalyst coating is considered as an alternative scheme in the micro-channel reactors.
但微通道尺度小,采用颗粒催化剂容易堵塞通道且压降较大,催化剂的利用率低,所以催化剂涂层的制备是微通道反应器发展的关键因素之一。
补充资料:涂胶
分子式:
CAS号:

性质:将胶浆(包括溶剂胶浆、胶乳和水胶浆)均匀地涂覆到织物表面上的工艺。涂胶方法有刮涂、辊涂、浸涂和喷涂四种。制造很薄的胶布(0.15mm以内),而又要求有较高耐透气性与耐水性时,适宜用涂胶法多次涂胶。若织物强度很小,经不起压延贴胶压力时,宜用涂胶法。织物先涂胶而后压延贴胶,可显著提高纤维与胶料的黏结力。按国家规定,生产车间空气中,汽油气体浓度不得超过0.3mg/L,当浓度达5~6mg/L时,可导致急性中毒。降低溶剂气体浓度最有效的方法是设置溶剂回收装置,并同时设有良好的通风装置。生产车间中的电动机、排风机及照明设备的电开关,都须全密闭式,以避免产生电火花。传动带、涂胶机、搅拌机等,均须安装有效的导静电设备及接地线路,并需有效的灭火器材,时刻注意防火防爆。