1) macroscopic streak flaw test
断面缺陷宏观检查
2) macroscopic defect
宏观缺陷
1.
The macroscopic defects of hydrothermal KTP crystal are mainly twin and coalescence crystal,growth spine,cracks and inclusions.
本文报道了水热法KTP晶体的生长工艺及晶体生长形态,系统研究了水热法KTP晶体的宏观缺陷,其宏观缺陷主要为添晶、生长脊线、裂隙和包裹体。
2.
The macroscopic defects of KBBF are mainly twin and coalescence crystal,inclusions,macrosteps,growth striations and cracks.
其宏观缺陷主要为连生、孪生、包裹体 ,宏观生长台阶和条纹、开裂等。
3) macroscopic defects
宏观缺陷
1.
The main macroscopic defects such as striations, side cores, bubbles, inclusions and stress birefringence were observed in as-grown Ce:YAG crystal by means of cross-polarized light microscope.
采用温度梯度法(TGT)成功生长了直径为76mm高光学质量的Ce:YAG高温闪烁晶体,采用偏光显微镜研究了Ce:YAG闪烁晶体中的主要宏观缺陷,观察到了生长条纹、侧心、气泡、包裹物以及应力双折射等宏观缺陷。
补充资料:点缺陷(见晶体缺陷)
点缺陷(见晶体缺陷)
point defect
点缺陷point defeet见晶体缺陷。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条