The location and shape of hearth and bottom erosion line of blast furnace can be calculated by a two-dimensional model set up with the boundary element method,and the erosion station of the furnace lining is known in time.
采用边界元方法建立某一大型高炉炉缸炉底的侵蚀推测二维模型,能够推定高炉炉缸炉底侵蚀线的位置和形状,及时了解炉衬侵蚀状态。
2.
It is indicated through the calculated erosion graph that erosion line at 1 150 ℃ is located in the fifth layer of carbon brick,that there is not big shape of "elephant foot",and that the erosion is quite normal.
通过对模型的计算,得到了炉缸炉底的温度场分布,从计算所得到的侵蚀图来看,1150℃侵蚀线位于第5层碳砖的位置,无明显的"象脚状"侵蚀,6号高炉炉缸炉底的侵蚀状况基本正常。
4)  Oilfield corrosion
管线腐蚀
5)  suture erosion
缝线侵蚀
1.
Prevention of postoperative suture erosion during transscleral fixation of posterior chamber intraocular lenses;
后房型人工晶状体缝线固定术后缝线侵蚀的预防
6)  corrosion wire breakage
腐蚀断线
1.
In order to solve the new contradiction and questions about lightning strike breakdown,insulation coordination,equipment selection,construction technology caused by overhead line distribution net newly built using the insulated conductor and old line insulation transformation,the article analyses thoroughly mechanism on lightning strike breakdown and corrosion wire breakage.
针对新网架空线路采用的绝缘导线和老线路的绝缘化改造带来的雷击断线及绝缘配合、设备选型及施工工艺等方面的新矛盾及问题,论文深入分析了雷电断线和腐蚀断线的机理,对比目前所采取技术手段的优缺点,结合线路现状,提出了采用过电压保护器进行改造的方法,详细论述了过电压保护器设备的选择和设备参数的选取,提出相应施工及技术改进措施。
补充资料:石油产品液相锈蚀试验
分子式:
CAS号:

性质:在规定条件下,将符合要求的钢棒浸入试样与蒸馏水或盐水(人工海水)的混合液中保持至规定时间后,目视钢棒的生锈程度的试验。当用人工海水时,也称为海水腐蚀试验。