1) cutting teeth of dredge bucket
泥斗斗齿
2) bucket teeth
斗齿
1.
Repair of welding rack for high Mn steel bucket teeth;
高锰钢斗齿焊接裂纹的修复
2.
Aimed at the wear phenomena of bucket teeth for great type mine excavators,the failure causes were analyzed based on tribology principle,some anti-wear measures were presented,such as improving the design,selecting materials rationally and surface disposal.
针对大型矿山挖掘机斗齿磨损失效现象,运用摩擦学原理,分析了失效原因,提出了通过改进设计、合理选材和表面处理等抗磨措施。
3) tooth
[英][tu:θ] [美][tuθ]
斗齿
1.
The cause of the crack and no-hardening happening in the low-alloy steel heavy section tooth casting in the condition of normal heat treatment process was analysed.
分析了低合金钢厚截面斗齿在常规热处理条件下易出现齿腔裂纹和齿尖淬不透的成因,提出了具体的热处理工艺方案,消除了PC1000和SKA006的淬火裂纹,并获得了良好的硬度和韧性。
4) dipper teeth
斗齿
1.
Castings quality control for bimetal composite dipper teeth;
双金属液复合浇注斗齿的铸件质量控制
2.
Hydraulic simulated test of transitional zone of dipper teeth for bimetal composite cast;
双金属液复合铸造斗齿的过渡区水力模拟试验
3.
Under the influence of numerous complex working conditions and soft media, the traditional high manganese steel (ZGMn13 )dipper teeth can not meet the demands of wear-resistance.
通过对低碳低合金钢的成份、热处理工艺、金相组织及机械性能的研究与分析,并借鉴国外斗齿的使用经验提出低碳低合金钢是抵抗高应力、高频率冲击载荷磨粒磨损工况条件下的理想耐磨材料之一。
5) Bucket Tooth
斗齿
1.
Manufacturing of Low-alloying Steel Bucket Tooth in Lost Foam Casting;
用消失模工艺生产低合金钢斗齿的试验研究
2.
Methods for promoting the life expectancy of high manganese steel bucket tooth;
提高高锰钢斗齿使用寿命的途径