1) needled paper-making felt
针刺造纸毛毯
2) paper maker felt needle loom
造纸毛毯针刺机
3) needled wet felt
针刺造纸湿毯
4) needle punching felt
针刺毛毯
5) mono-filament net needling paper felt
单丝底网针刺造纸毯
6) papermaking felt
造纸毛毯
1.
The purpose,principle and methods of permeability testing of papermaking felt are introduced.
介绍了造纸毛毯透通性等性能测试的目的、原理和方法,分析了造纸毛毯透气性、透水性、含水量之间的关系及其对毛毯运行性能的影响;探讨了造纸毛毯透通性等性能测试方法的发展趋势。
2.
On the basis of analyzing the water filterability, the research on the soil-release finish of papermaking felt are made.
以滤水性能的变化为依据 ,对造纸毛毯的抗污整理进行了研究 ,同时也对造纸毛毯抗沾污性能的测试方法进行了探索。
3.
This paper introduces the standard for Chinese papermaking felt industry and the experience in execution, then puts forward the additional technical requirements for the modern papermaking felt and the demanding for farther reseach and formalating a higher standard.
介绍我国造纸毛毯行业标准和执行该标准的体会 ,提出现代造纸毛毯应具有的现行标准所未包含的其他技术要求以及加快研究和制订更高造纸毛毯标准的意
补充资料:造纸毛毯
造纸机上使用的毛毯。按照在造纸机上的部位可分为湿毯、上毯和干毯。湿毯在造纸机上带水运转,作用是压榨纸坯使之脱水和纸面平滑。湿毯滤水性和弹性都好,强度高,收缩率小,耐磨,能抗细菌和抗酸碱腐蚀。上毯使用部位在湿毯的上方,有小部分接触烘缸,起领纸、顶平和干燥的作用,具有平整、硬挺、弹性好、耐磨、耐高温的性能。干毯包覆烘缸,在湿热和干燥状态下运行,对纸张起熨平和烘干作用,具有坚实、弹性好、耐磨、耐高温的性能。干毯也可以帆布或用涤纶长丝织制的透气性织物来代替。造纸毛毯分机织和针织两种。机织造纸毛毯采用羊毛和锦纶短纤维混纺纱线,混纺比约为 75:25,经织造、缩呢、起毛、烘干定型等工序制成。针刺造纸毛毯的制造方法是先将50%羊毛和50%锦纶短纤维或100%锦纶短纤维梳理成纤维网,多层重叠,再用带倒刺的钢针把纤维网刺到预先织好的环形底布上,达到一定的紧密度和平整度。针刺的方法有单面针刺和双面针刺。针刺毛毯具有滤水性好、耐磨、强度高、使用寿命长的特点。