1)  strain crack;strain cracking
应变裂纹
2)  strain to fracture
应变-裂纹(STF)试验
3)  principal strain/twist angle of crack plane
主应变/裂纹面扭转角
4)  stress
应变
1.
Meso-mechanical analysis has been conducted with finite element for a hot-rolled steel of 16MnR to investigate the effect of the elongated pre-damage voids on the subsequent damage evolution and fracture process under multidirectional maximum normal stresses.
结果表明:热轧钢中的长条形夹杂物与基体剥离后形成的长条形孔洞在后续加载中,其周围产生的局部高应力应变集中及其相互作用使孔洞长大。
2.
It analyses the strain and the stress in drawing, the existing questions of drawing technology at present, the critical condition of losing stability, the effect on products' quality and drawing die, and the status of the remaining strain.
 比较了不锈钢产品与普通低碳钢产品在拉深过程中的异同,分析了产品成形过程的应力应变状态、现行拉深工艺存在的问题、不锈钢薄板拉深失稳的临界条件以及失稳起皱对拉深件质量和模具的影响和拉深件的残余应力状态。
3.
In order to determine the optimal shape of interchamber pillars,seven models are established using finite element numerical simulation technique to study the influence of different orebody dip angles and different intersection angles between the normal lines of pillar wall and ore bed on pillar strain and stress.
本文采用有限元数值模拟技术,建立了七种模型,计算分析了不同矿体倾角及矿柱壁面与矿层面法线夹角的变化对矿柱应力应变状态的影响,从而确定出最佳的矿柱形状。
5)  strain
应变
1.
Effect of strain on the electrical resistance of continuous carbon fiber monofilament;
连续碳纤维单丝的应变电阻效应
2.
Research on the stress and strain evolution of aluminum alloy hot forging die;
铝合金热锻模具结构中的应力应变演变过程分析
3.
Analysis on Stress and Strain Behavior of Spherical Vessel of Functionally Graded Material under Creep Condition;
蠕变条件下梯度材料球罐应力应变行为分析
6)  deformation
应变
1.
Analog computation of the deformation of continuously casted bloom in secondary cooling zone;
连铸大方坯二次冷却区域两相界应变的模拟计算
2.
When the burring process of 12×4J wheel is processed taking the deformation area as the plane stress condition,the deformation characteristics of normal and radius directions are studied,which is influenced by the factors such as height and the inner hole initial radius and the deformation law of circle strain.
利用斜冲模对12×4J轮辐进行翻边时,将变形区看做是平面应力状态,探讨了翻边高度、初始孔径及斜冲模角对翻边变形区径向应变和轴向应变的影响,对12×4J轮辐翻边不同斜冲模角下的冲压力变化规律进行了计算。
3.
It focuses on demonstrating special characteristic of prestress and inside dint of the concrete;At the same time,the stress and deformation to the beam construction is examined.
针对东海大桥主跨420 m的钢混凝土箱形结合梁斜拉桥中一片主梁进行了工艺试验研究,分析了混凝土的预应力和内力均在变化的特殊性;同时,对结构的应力、应变进行了检测。
参考词条
补充资料:淬火裂纹和非淬火裂纹的特征及实例分析

淬火裂纹是指在淬火过程中或在淬火后的室温放置过程中产生的裂纹。后者又叫时效裂纹。造成淬火开裂的原因很多,在分析淬火裂纹时,应根据裂纹特征加以区分。


一、淬火裂纹的特征


在淬火过程中,当淬火产生的巨大应力大于材料本身的强度时,便会导致裂纹产生。淬火裂纹往往是在马氏体转变开始进行后不久产生的,裂纹的分布则没有一定的规律,但一般容易在工件的棱角槽口、截面突变处形成。


在显微镜下观察到的淬火开裂,可能是沿晶开裂,也可能是穿晶开裂;有的呈放射状,也有的呈单独线条状或呈网状。


因在马氏体转变区的冷却过快而引起的淬火裂纹,往往是穿晶分布,而且裂纹较直,周围没有分枝的小裂纹。


因淬火加热温度过高而引起的淬火裂纹,都是沿晶分布,裂纹尾端尖细,并呈现过热特征:结构钢中可观察到粗针状马氏体;工具钢中可观察到共晶或角状碳化物。


表面脱碳的高碳钢工件,淬火后容易形成网状裂纹。这是因为,表面脱碳层在淬火冷却时的体积胀大比未脱碳的心部小,表面材料受心部膨胀的作用而被拉裂呈网状。


二、非淬火裂纹的特征


淬火后发生的裂纹,不一定都是淬火所造成的,一般可根据下面的特征来区分。


淬火后发现的裂纹,如果裂纹两侧有氧化脱碳现象,则可以肯定裂纹在淬火之前就已经存在。淬火冷却过程中,只有当马氏体转变量达到一定数量时,裂纹才有可能形成。与此相对应的温度,大约在250℃以下。在这样的低温下,即使产生了裂纹,裂纹两侧也不会发生脱碳和出现明显氧化。所以,有氧化脱碳现象的裂纹是非淬火裂纹。


如果裂纹在淬火前已经存在,又不与表面相通,这样的内部裂纹虽不会产生氧化脱碳,但裂纹的线条显得柔软,尾端圆秃,也容易与淬火裂纹的线条刚健有力,尾端尖细的特征区别开来。


三、实例分析


实例一:


40Cr钢制成的转子轴,经锻造、淬火后发现裂纹。裂纹两侧有氧化迹象,经金相检验,裂纹两侧存在脱碳层,而且裂纹两侧的铁素体呈较大的柱状晶粒,其晶界与裂纹大致垂直。结论:裂纹是在锻造时形成的非淬火裂纹。


当工件在锻造过程中形成裂纹时,淬火加热即引起裂纹两侧氧化脱碳。随着脱碳过程的进行,裂纹两侧的碳含量降低,铁索体晶粒开始生核。当沿裂纹两侧生核的铁素体晶粒长大到彼此接触后,便向离裂纹两侧较远的基体方向生长。由于裂纹两侧在脱碳过程中碳浓度的下降,也是由裂纹的开口部位向内部发展,因而为铁素体晶粒的不断长大提供了条件,故最终长大为晶界与裂纹相垂直的柱状晶体。