2) oxidation aging
氧化老化
3) Photooxidation aging
光氧老化
1.
Study on photooxidation aging apparent viscosity of asphalt
光氧老化对沥青表观粘度的影响
2.
From the experiments of short-term aging(Rolling Test of Film Oxidation(RTFO))and photooxidation aging of AH-70 original asphalt and SBS PG76-22 modified asphalt,this paper examined the effects of UV-light on asphalt by using FI-IR theory.
通过AH-70基质沥青及PG76-22改性沥青的短期热氧老化(RTFO)和模拟光氧老化试验,运用红外光谱分析法研究真实环境中太阳光中紫外光对沥青胶结料的影响。
4) thermal oxidative aging
热氧老化
1.
Effect of OMMT on thermal oxidative aging of PPC/OMMT nanocomposites was investigated.
研究了OMMT对PPC/OM-MT纳米复合材料热氧老化的影响。
2.
The influence of 4010NA antioxidant powder and traditional 4010NA antioxidant on the vulcanizing characteristics, thermal oxidative aging stability under free condition, and water extraction resistance of NR compounds were investigated.
研究了粉状防老剂4010NA与普通防老剂4010NA对NR胶料的硫化特性、自由状态下的热氧老化防护性能及耐水抽出性的影响。
3.
A comparative test of new antioxidants 350 and PS 988 to traditional antioxidants A,D,RD and 4010NA in NR compound was made in terms of thermal oxidative aging property,flex cracking,cut growth resistance and weathering resistance,and their effect on the curing rate of NR compound was investigated.
在NR中进行了新型防老剂 35 0和PS 988与传统防老剂A ,D ,RD和 40 10NA的热氧老化、抗屈挠龟裂与抗裂口增长及大气老化对比试验 ,并研究了对NR胶料硫化速度的影响。
5) thermo-oxidative aging
热氧老化
1.
Properties of stress relaxation and compression set of vulcanite during isothermal thermo-oxidative aging
硫化胶等温热氧老化时应力松弛和压缩永久变形性能的研究
2.
Three kinds of clay were treated by using reductant, strong acid and additionalmetal compounds, and the corresponding clay/rubber masterbatch was prepared for testing theproperties of thermo-oxidative aging.
通过还原剂、强酸及添加金属化合物的方法处理3种粘土,并制备相应的粘土胶进行热氧老化性能测试。
3.
The hardness, elongation at break, tensile strength, modulus, compression stress relaxation and permanent compression set of the rubber vukanizates in thermo-oxidative aging were described.
循此基本规律可预测橡胶及其制品的贮存或使用寿命,建立橡胶耐热氧老化性的合理评定方法,以及构成常温叠合曲线来研究弹性体长时间的粘弹性行为。
6) photooxidative aging
光氧老化
1.
Affect of nano-Ti on photooxidative aging-resistant properties of PP;
纳米钛对PP耐光氧老化性能的影响
2.
The effect of photooxidative aging on the physical propertier of polyethylene(PE) film was stu died.
研究了光氧老化过程对聚乙烯薄膜物理性能的影响 ,对比考察了光稳定剂对不同种类、不同厚度聚乙烯薄膜耐光氧老化性能的影响。
补充资料:天候氧老化试验仪
分子式:
CAS号:
性质:测定橡胶耐候、耐氧老化性能的仪器,其主体为备有鼓风、喷雾和控温功能的烘箱,烘箱内还安装有用于夹持试样的转鼓和模拟自然光的碳弧灯。试验时将试样装在转鼓上绕碳弧灯旋转,在接受辐射能的同时,每间隔一定时间由喷雾器进行降雨,进而送风调温,使之经受和室外类似的老化条件进行试验。