1) inside mandrel
内芯棒
2) mandrel
[英]['mændrəl] [美]['mændrəl]
芯棒
1.
Modifications of Mandrel Cooling System and Outlet Table of Assel Pipe Mill;
Assel轧管机芯棒冷却及后台设备的改造
2.
Discussion on Optimizing Deformation Process to Enhance Mandrel Utilization Factor;
优化变形工艺提高芯棒利用效率的探讨
3.
3D finite element analysis of effect of mandrel on continuous seamless tube rolling process;
芯棒对连轧管轧制过程影响的三维有限元分析
3) core
[英][kɔ:(r)] [美][kɔr]
芯棒
1.
Through tests of ACCC under different high temperature conditions,it is found that under high temperature,the surface of carbon fiber composite core of strain jumper section will appear something like "bamboo knots",which requires special attention in design.
但也有其自身的弱点,通过对ACCC导线进行不同状态的耐高温性能试验,发现该导线耐张跳线段的碳纤维复合芯棒表面高温运行时会出现"竹节"现象,在设计中应予特别关注。
2.
The effect of pressing procedure on mechanical property was investigated with different core,stress and production procedure.
介绍了国内外棒形悬式复合绝缘子金属附件连接区的设计结构,从不同厂家芯棒、压接力和生产工序三方面研究了连接区采用压接式结构对产品机械性能的影响,提出了在设计连接区时应考虑圆度、连接区的长度、端口的密封性、压块的长度及壁厚等因素。
4) Core rod
芯棒
1.
Cause study and countermeasures for core rod brittle fracture of suspension composite insulators on 220kV Ping-He line;
220kV坪核线复合绝缘子芯棒脆断原因分析及对策
2.
By analyzing the damage of the core rod and the sheath,the causations of the fault are analyzed.
介绍了500kV北增甲线59号塔L2相双V形复合绝缘子串断裂的故障情况,通过分析芯棒和护套的受损形貌,指出故障形成的主要原因是复合绝缘子受到局部放电腐蚀和化学腐蚀而使机械强度降低,次要原因是均压环结构设计不合理。
5) retained mandrel
限动芯棒
1.
Production practice of applying DRI in steelmaking for retained mandrel steel;
直接还原铁在限动芯棒钢冶炼中的生产实践
2.
Discussion on the design method of diameters of series of mandrels of retained mandrel mill;
限动芯棒连轧管机芯棒直径系列的设计方法
3.
The quality of seamless tube can be improved greatly by using retained mandrel mill with on line inspection This paper summarizes the practice of retained mandrel mill at TPCO (Tianjin Pipe Corp ), and a detailed analysis of technical difficulties and major product defects were given with proposed the precaution measure
采用限动芯棒连轧工艺生产无缝钢管,再加上先进的在线检测技术,使得无缝钢管产品的质量有了可靠的保证。
6) H13 steel core bar
H13钢芯棒
1.
After quenching and tempering, material H13 steel core bar was broken during alignment There are naphthalene fractures on macroscopical fractures surface.
H13钢芯棒毛坯在调质热处理后的校正工序中发生断裂,宏观断裂面出现萘状断口。