4)  pit [英][pɪt]  [美][pɪt]
麻点
1.
Cause and settlement measure of pitting during hard chromium plating;
镀硬铬出现麻点的原因及对策
2.
Causes and trouble-shootings for pores and pits on nickel electrodeposits;
镀镍层针孔和麻点的故障及其排除方法
3.
Having pits on deposits is the common defect in electroplating processing.
 镀层麻点是电镀加工的常见质量问题。
5)  pock [英][pɔk]  [美][pɑk]
麻点
1.
According to the discussion about comentite gears picked surface,the author points out the main reasons of pock gears surface in the heat treatment process are the quality of salt and the improper operation.
通过对齿轮在热处理过程中产生“麻点”缺陷原因的探析,指出热处理过程中盐的质量和操作不当及渗碳过程是产生“麻点”的主要原因,其本质都属于不完全氧化所产生的腐蚀,并提出了简明的预防方法。
2.
As for pocks exist on the surface of the plates,I ve taken multi-angle analyse and study about this kind of defect, among clearing exterior steel billet,heating technics,forming oxidation steel iron,in addition,influence elements,the results of removing squama through high pressure water and factors about removing squama.
针对南钢中板厂中厚钢板表面麻点缺陷的特点,对其产生原因从钢坯表面的清理、加热工艺、氧化铁皮的生成和影响生成的因素、高压水除鳞的效果和影响除鳞效果的因素等多方面进行了分析和研究。