1) W-type strontium ferrites
W型锶铁氧体
1.
W-type strontium ferrites are prepared by citric acid sol-gel method.
采用柠檬酸溶胶-凝胶法制备了W型锶铁氧体SrZn_2Fe_(16)O_(27),研究了制备过程中柠檬酸用量、溶液pH、煅烧温度以及煅烧时间对纳米晶性能的影响。
2) W-type ferrite
W型铁氧体
1.
Study on preparation and electromagnetic properties of W-type ferrites doped with nickel
镍掺杂W型铁氧体的制备及电磁性能研究
2.
When calcination temperature was 1250~1300℃,the product was single W-type ferrite.
结果表明,煅烧温度低于1200℃时,产物为M晶型的铁氧体;煅烧温度为1250~1300℃时,生成单一的W型铁氧体;温度1350℃时,产物中生成了少量M晶型铁氧体。
3) W-ferrite
W-型铁氧体
5) strontium ferrite
锶铁氧体
1.
Preparation of strontium ferrite powder by iron concentrate and its sintering dynamics;
用超纯铁精矿生产锶铁氧体预烧料及其焙烧动力学
2.
Powder injection molding(PIM) was applied to make radially oriental magnetic rings of strontium ferrite.
应用粉末注射成型(PIM)烧结技术制备了锶铁氧体辐射环,并对其微观组织、磁性能、脱脂及烧结工艺进行了研究。
3.
In this paper, the influence of the sintering temperature and thermostatic time on the magnetic properties and structures of strontium ferrite is studied.
研究了锶铁氧体烧结过程中烧结温度、恒温时间对锶铁氧体磁性能及结构的影响。
6) W-type barium ferrite
W型钡铁氧体
1.
Effect of rare earth substitution on microwave-absorbing properties of W-type barium ferrite;
稀土元素对W型钡铁氧体微波吸收特性的作用
2.
The samples of La-doped W-type barium ferrite Ba1-xLaxCo2Fe16O27(x=0,0.
用溶胶-凝胶法制备镧掺杂W型钡铁氧体Ba1-xLaxCo2Fe16O27(x=0,0。
补充资料:锶铁氧体
CAS:12023-91-5
分子式:Fe12O19·Sr
熔点:450℃
中文名称:氧化硒铁;锶铁氧体
英文名称:Iron strontium oxide;ferrate, strontium;strontium dodecairon nonadecaoxide;strontium-iron oxide
分子式:Fe12O19·Sr
熔点:450℃
中文名称:氧化硒铁;锶铁氧体
英文名称:Iron strontium oxide;ferrate, strontium;strontium dodecairon nonadecaoxide;strontium-iron oxide
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条