1) HET resin
HET 酸树脂
2) HET-acid
HET酸
1.
The study was made on the synthesis and properties of HET-acid type UP modified with epichlorohydrin.
本文研究了以环氧氯丙烷为端基封闭剂改性HET酸型不饱和聚酯树脂的合成和性能,讨论了环氧氯丙烷含量对树脂性能的影响,利用差热分析(DTA)、热重分析(TG)对改性树脂的热分解过程进行了初步的讨论。
3) resinate
[英]['rezineit] [美]['rɛzɪ,net]
树脂,酸脂
4) resin acid
树脂酸
1.
The main components which can cause pitch trouble in the process of paper making with Masson pine TMP was simulated by using fatty acid,resin acid and oleic triglyceride as model materials.
以脂肪酸、树脂酸、三油酸甘油脂为模型物,模拟了马尾松TMP造纸过程中造成树脂障碍的主要成分。
2.
Nano-Ni was first used as catalyst for disproportionation of resin acid.
将纳米镍催化剂首次应用于树脂酸的歧化反应中。
3.
The morphological variation characteristics of resin acid,as well as titration correction of the unsaponifiable matter during rosin saponification were discussed theoretically.
研究了在脂松香分析测定过程中影响松香不皂化物含量测定的关键因素及其影响机理,讨论了树脂酸在皂化过程中的形态变化特征及其导致不皂化物需要进行树脂酸校正操作和计算的理论依据。
5) acid-sensitive resin
酸敏树脂
6) zinc resinate
树脂酸锌
补充资料:HET
氯茵酸酐又称氯桥酸酐、六氯内次甲基四氢邻苯二甲酸酐,简称HET、CA,分子量370.9白色晶粉末,熔点240~24l ℃。含氯量57.4%,溶于丙酮、苯、微溶于正已烷、四氯化碳。在水中水解为氯桥酸。
用作环氧树脂的固化剂,参考用量100~110phr。固化条件l00 ℃/2h十160℃/4h或120℃/2h十180℃/4h或100℃/1h十160 ℃/4h十200 ℃/1h。固化物具有优良的阻燃性、电性能和机械性能。热变形温度181℃。
用作环氧树脂的固化剂,参考用量100~110phr。固化条件l00 ℃/2h十160℃/4h或120℃/2h十180℃/4h或100℃/1h十160 ℃/4h十200 ℃/1h。固化物具有优良的阻燃性、电性能和机械性能。热变形温度181℃。