2) micro-stage grinding
微阶段化磨矿
1.
Influencing factors of the micro-stage grinding technique
微阶段化磨矿技术效果的影响因素
3) stage-wise grinding
阶段磨矿
1.
At present,two kinds of flowsheets are adopted in Qidashan Beneficiation Plant-"stage-wise grinding-gravity separation,magnetic separation and anion reverse flotation" and"continuous grinding-low intensity magnetic separation,high intensity magnetic separation and anion reverse flotation".
目前选别齐大山铁矿石的工艺流程分别为"阶段磨矿、重-磁-阴离子反浮选"和"连续磨矿、弱磁-强磁-阴离子反浮选"。
2.
It is then determined that the flowsheet of stage-wise grinding—gravity separation—high intensity magnetic separation-anion reverse flotation is most reasonable for beneficiation of poor hematite from Gongchangling Mine.
在对弓长岭贫赤铁矿石性质研究的基础上, 从合理工艺流程的角度对试验数据进行分析, 确定阶段磨矿、重选 强磁 阴离子反浮选工艺流程为处理弓长岭贫赤铁矿的合理流程。
4) Stage grinding
阶段磨矿
1.
Based on process mineralogical characteristics of villaninite,a process of "stage grinding,stage flotation,and concentrate discharge from two points" was adopted.
根据该硫化铜镍矿的工艺矿物学特点,采用阶段磨矿、阶段浮选、两点出精矿的选矿流程。
2.
The experimental studies on stage grinding and leaching of high sulfurcontaining gold concentrate of Rusan District are made.
对乳山地区高硫金精矿进行了阶段磨矿、阶段浸出的试验研究。
3.
After the process mineralogical study and beneficiation experiments on ores from Dagushan and Yanqianshan,and lean magnetite ore from Gongchangling,it is concluded that a process consists of stage grinding,single magnetic separation,and fine screening-regrinding is technically advanced and feasible in treating lean magnetite ores from Anshan.
通过大孤山矿石、眼前山矿石及弓长岭贫磁铁矿石的工艺矿物学研究和选别试验研究,认为采用"阶段磨矿,单一磁选-细筛再磨流程"处理鞍山贫磁铁矿石是先进的、合理的。
5) Staged grinding
阶段磨矿
1.
78% iron was separated in the laboratory by using the craft flow of staged grinding and classification-gravity separation-magnetic separation-anionic reverse flotation.
通过实验室采用“阶段磨矿、粗细分级、重选—磁选—阴离子反浮选”工艺流程处理某地贫赤铁矿取得原矿品位30。
6) mineralization stage
矿化阶段
1.
Based on EPMA analysis of arsenopyrite and the phase diagram of coexisting minerals pyrite-arsenopyrite,we conclud that temperature of the main mineralization stage is stable within 300~450℃.
本文通过主要矿化阶段热液矿物毒砂成分的测定,利用相图中共生金属硫化物稳定温度范围得出主要矿化阶段的温度为300~450℃,它比通过石英流体包裹体测得的均一温度更准确地代表成矿流体的温度,由此温度平均值计算出的氢氢同位素能准确判断初始流体的来源。
补充资料:分段落矿阶段矿房采矿法
分段落矿阶段矿房采矿法
block open stoping with ground breaking from sublevel
fenduan luokuongJ一ed旧n kLJangfang eo一kuangfo分段落矿阶段矿房采矿法(bloek open stop-ing with ground breaking from sublevel)划矿房为分段,自各分段巷道用上向扇形或环形中深孔或深孔落矿的阶段矿房采矿法。结构参数和采准矿体厚度小于15或20m时,矿块沿矿体走向布置矿体再厚时,矿块垂直矿体走向布置。沿矿体走向布置的分段落矿阶段矿房采矿法的结构参数和采准巷道位置见图。分段高度取决于所用凿岩设备钻凿炮孔的有效深度用Y(;Z一90型凿岩机时,分段高度多为IOm,用YQ一1。。型钻机时,分段高度多为15m。为了不凿过深的孔,把分段巷道布置在靠近矿体下盘侧。掘进分段巷道时多用电把出碴。注一月 B~.州卜一月 无尸丫夕飞夕夕)勺生乙二乙之二恋花〕月左已乙龙色飞几汪二二二日 志卜‘+‘沙卜‘斗分“卜卜月份“飞104、人乍气r叮,二下吸飞 卜一一止穿写月’7卜“ 〔’一〔-峨苹卿哪 分段落矿阶段矿房采矿法 1崩落岩石;2一矿务;3间柱;4一底柱:5、6、7分别为脉外、脉为和穿脉运输巷道;吕人行通风天井9联络巷道;l。原切割槽;11一分段凿岩巷道; 12炮孔1污落下护石11漏斗:]几一把扩巷道;16溜井切割和回采切割包括拉底,扩漏和拉各分段的切割槽。多用中深孔自上而下分段拉槽。拉底高度为2一25。,多用浅眼进行。从漏斗天井凿上向浅眼和从拉底水平凿下向浅眼爆破扩漏。拉底和扩漏超前于回采落矿自由面一个漏斗。回采工作包括:在各个分段中凿中深孔或深孔,凿完全部中深孔或深孔后,逐排爆破,落卜矿石借重力溜至耙矿巷道,用电耙运搬至溜井中。在中国,主要用YGZ一90型凿岩机凿上向扇形中深孔或用YQ一l。。型钻机凿上向扇形深孔。其他国家的一些矿山用潜孔钻机凿环形深孔或用液压凿岩台车凿环形中深孔。中深孔和深孔的最小抵抗线分别为1.5一1.sm和2.5一3n,,一次爆破3一5排。上下分段的爆破自由面在一个垂直面上,或者.为使上分段进行爆破作业安全,可使上分段的爆破自由面超前下分段l排炮孔。利用全矿总风流对各个回采作业地点通风 适用条件适用于矿岩稳固的急倾斜中厚和厚矿体,要求矿体形状较规则,矿体含夹石少,矿石品位较均匀。评价与垂直深孔阶段矿房采矿法相比,分段落矿阶段矿房采矿法采准工作量大,但控制矿体边界容易。