说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 异常区分
1)  anomaly distinguish
异常区分
2)  distinction between anomalies
区分异常
3)  gas abnormal distribution area
瓦斯异常分布区
1.
restrict the gas content of the coal seam, introduces the classification of the gas emission, and analyzes on the situations of the gas abnormal distribution area of 12#coal seam of Guzhuang Coal Mine and gets some useful conclusions.
指出围岩透气性、地质构造、煤层埋藏深度、地下水活动情况等因素综合影响而形成的储气条件制约了煤层中的瓦斯含量,介绍了瓦斯喷出(突出)的分类,分析了固庄煤矿12#煤层瓦斯异常分布区的状况并得出了有用的结论。
4)  anomaly property distinction
异常性质区分
5)  abnormal area
异常区
1.
3 abnormal area at the Wutongzhuang coal mine,the resulting data shows that in this area exists a group of in-development mini-faults,with fault water channeling instead of collapsing column water transmitting.
运用三维天然电磁波勘探法在地面对开采的峰峰矿区梧桐庄矿3号异常区进行探测,资料解释结果表明:3号异常区存在一组发育的小断层,为断层导水,而不是陷落柱导水。
6)  Regional Anomaly
区域异常
1.
The estimation of regional anomaly is obtained under the conditions of linear, unbiased and.
在重(磁)资料的分析处理中,经常需要划分区域异常与局部异常。
补充资料:共析钢、亚共析钢、过共析钢区分介绍
碳溶解在铁的晶格中形成固溶体,碳溶解到α——铁中的固溶体叫铁素体,溶解到γ——铁中的固溶体叫奥氏体。铁素体与奥氏体都具有良好的塑性。当铁碳合金中的碳不能全部溶入铁素体或奥氏体中时,剩余出来的碳将与铁形成化合物——碳化铁(Fe3C)这种化合物的晶体组织叫渗碳体,它的硬度极高,塑性几乎为零。
1.共析钢
从反映钢的组织结构与钢的含碳量和钢的温度之间关系的铁碳平衡状态图上可见,当碳的含量正好等于0.77%时,即相当于合金中渗碳体(碳化铁)约占12%,铁素体约占88%时,该合金的相变是在恒温下实现的。即在这种特定比例下的渗碳体和铁素体,在发生相变时,如果消失两者同时消失(加热时),如果出现则两者又同时出现,在这一点上这种组织与纯金属的相变类似。基于这个原因,人们就把这种由特定比例构成的两相组织当作一种组织来看待,并且命名为珠光体,这种钢就叫做共析钢。即含碳量正好是0.77%的钢就叫做共析钢,它的组织是珠光体。
2.亚共析钢
常用的结构钢含碳量大都在0.5%以下,由于含碳量低于0.77%,所以组织中的渗碳体量也少于12%,于是铁素体除去一部分要与渗碳体形成珠光体外,还会有多余的出现,所以这种钢的组织是铁素体+珠光体。碳含量越少,钢组织中珠光体比例也越小,钢的强度也越低,但塑性越好,这类钢统称为亚共析钢。
3.过共析钢
工具用钢的含碳量往往超过0.77%,这种钢组织中渗碳体的比例超过12%,所以除与铁素体形成珠光体外,还有多余的渗碳体,于是这类钢的组织是珠光体+渗碳体。这类钢统称为过共析钢。