In order to examine the action characteristics of the potassium titanate whisker and ramie fiber in polypropylene,the orthogonal experiment design was used,and the polypropylene composite reinforced by the potassium titanate whisker and ramie fiber was prepared by means of the torque rheometer blending and transfer molding.
为了考察苎麻纤维和钛酸钾晶须混杂增强聚丙稀时的行为特征,采用正交实验设计、转矩流变仪共混和传递模压成型技术研制了苎麻和钛酸钾晶须混杂增强聚丙稀复合材料,并通过方差和极差分析方法对材料的强度和韧性指标进行了研究。
2.
The paper introduces the principle, character and application of the powder static electricity eliminating meter in packing polypropylene.
在聚丙稀粉体生产过程中 ,静电荷聚积所产生电击或静电火花 ,可能引起对人体伤害和生产事故等隐患 ,文章介绍了AJS -2系列粉体静电消除器的主要组成原理及技术特点 ,该仪器 2 0 0 0年至今在河南油田聚丙稀放料及整个生产过程中的应用效果表明 ,采用消电装置使聚丙稀粉体静电位由原来最高 6 0kV ,最低 5kV ,平均在 2 5kV左右 ,降到 0 。
5)  acrylamide
丙稀酰胺
6)  acylic acid
丙稀酸
1.
Phenolic resin is prepared by means of ring-opening reaction of epoxy phenolic resin with acylic acid,which resin can be cured by ultraviolet and can be used as bond in coated abrasives.
本文通过丙稀酸与环氧酚醛树脂开环反应,制备出能紫外光固化的酚醛树脂结合剂,研究了制备该树脂的合适工艺条件为:催化剂N,N-二甲基苯胺的用量为体系总质量的1%,反应温度为80±5℃,反应时间为5~7h;用这种可紫外光固化的酚醛树脂制作的涂附磨具试样,不仅固化速度快,仅需4~5m in即可固化完全,而且磨削比是常规热固化试样的3倍多,使用性能大大提高。
参考词条
补充资料:丙稀醇
   分子式  CH2=CHCH2OH
     分子量   58.08
    CAS号  107-18-6
    性质  具有刺激性芥子气味的无色液体。相对密度0.8520(20/4℃)。凝固点-129℃。沸点96.9℃。临界温度271.9℃。闪点(闭杯)22.2℃。在-190℃时变成玻璃体。折射率nD(20℃)1.4132。与水、乙醚、乙醇、氯仿和石油醚混溶。
  用途  用作医药、农药、香料的中间体, 也是邻苯二甲酸二烯丙酯树脂的原料
  毒性   有特殊臭味,且能强烈地刺激眼、皮肤、咽喉、粘膜,严重时可致失明。附着在皮肤上能使之发红而产生烫伤,并迅速经皮肤吸收,而引起肝脏障碍、肾炎、血尿等症状。毒性最强的醇之一,大鼠经口LD50为64mg/kg。狗经口LD50为40mg/kg。生产现场空气中最高容许浓度5mg/m3,在此浓度下刺激性已很强,无法长时间忍耐。当溅及皮肤时宜用水冲洗并涂油脂类药物。操作时穿戴防护用具。 
   包装储运  采用白铁桶包装。按易燃有毒物品规定贮运。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。