,the tensile and compressive strains due to relevant stress distributions in pre-stretched thick aluminum plate.
将求得的应力与初始已知的应力相比较,发现两者能很好地吻合,说明该方法可以用于预拉伸铝合金厚板内部残余应力的测量。
2)  pre-stretched aluminum alloy plate
铝合金预拉伸板
1.
The residual stresses in the pre-stretched aluminum alloy plate 7075T7351 are measured by using the crack-compliance method, and the distribution regularity of the residual stresses is analyzed in detail.
运用裂纹柔度法测量了铝合金预拉伸板 70 75T735 1的内部残余应力 ,分析了内部残余应力的分布规律 ,并测出厚度为 4 0mm的板长度方向最大残余拉应力为 18 3Mpa ,最大残余压应力为 17 9Mpa。
3)  pre-stretched thick plate
预拉伸厚板
1.
Effect of one-step ageing on microstructure and properties of 7B04 pre-stretched thick plate;
单级时效对7B04预拉伸厚板组织和性能的影响
2.
The microstructure and properties of two-step aged 7B04 aluminum alloy pre-stretched thick plate were investigated using TEM,tensile and electrical conductivity test.
研究了双级时效处理对7B04铝合金预拉伸厚板的组织和性能的影响。
4)  aluminium alloy plate
铝合金厚板
1.
Review about supply and demand of global aluminium alloy plate for aviation;
全球航空级铝合金厚板供需述评
5)  thick plate of aluminum alloy
厚板铝合金
1.
In this paper,the bead puckering during high current metal-inert-gas shield welding process of thick plate of aluminum alloy is analyzed.
对大电流MIG焊焊接厚板铝合金时焊缝产生皱皮进行了试验研究与分析,皱皮产生的原因是焊接电弧燃烧不稳定、熔池中的熔融金属发生氧化和氮化反应造成的。