1) Anodic Alumina Membranes(AAM)
阳极氧化铝模板(AAM)
2) anodic alumina membranes (AAM)
阳极氧化铝膜(AAM)
3) Anodic alumina membr ane (AAM)
氧化铝模板(AAM)
4) Anodic aluminum oxide template
阳极氧化铝模板
1.
By using anodic aluminum oxide templates,CoFe_2O_4 nanotubes were synthesized by chemical method.
利用阳极氧化铝模板,用化学方法合成了CoFe2O4纳米管。
2.
The anodic aluminum oxide templates were prepared with 0.
3 mol/L草酸作电解液,采用高电压制备阳极氧化铝模板,可以提高制备速度。
3.
The nickel nanowires with about 40-70nm in diameter is prepared on the ordered anodic aluminum oxide template by PLD.
在制备出的阳极氧化铝模板上利用激光脉冲沉积法制得了直径为40 nm~70 nm的镍纳米线,将镍纳米线涂在载玻片上作为基底,可以测得很强的苏丹红Ⅱ的表面增强拉曼散射光谱和尖端增强拉曼散射,扩大了表面增强拉曼散射的应用范围,也表明它存在着新的增强方式。
5) AAO template
阳极氧化铝模板
1.
Then, arrays of manganese dioxide nanowires were prepared using AAO template above by sol-gel method with a sol-gel solution containing Mn(CH_3COO)_2 and citric acid.
5M硫酸和 5g L草酸混合溶液中制得多孔氧化铝膜 ,经 5wt%的磷酸扩孔处理得到具有孔径大小均一 ,排列有序 ,并具有一定厚度的阳极氧化铝模板 (AAO) ,以该氧化膜为模板 ,用溶胶 凝胶法在其微孔内合成了MnO2 纳米线。
2.
In this paper, we prepared cobalt-iron alloy nanowires with AAO templates through pulse electrodeposition, and obtained the hard magnetic materal CoFe_2O_4 nanowires by further thermal oxidation.
本文首先通过脉冲电沉积法在阳极氧化铝模板中成功制备了CoFe_2软磁材料纳米线,然后经高温氧化处理得到硬磁材料CoFe_2O_4纳米线。
6) anodic aluminum oxide(AAO) template
阳极氧化铝模板
1.
High orderly CoPt nanowires arrays with diameter of 50 nm was fabricated successfully by electro-deposition in the anodic aluminum oxide(AAO) template.
用电化学沉积法,在阳极氧化铝模板(AAO)中成功制备了直径为50 nm的CoPt合金纳米线的高度有序阵列。
补充资料:银阳极泥提银(见铜阳极泥提金银)
银阳极泥提银(见铜阳极泥提金银)
extraction of silver from silver anode slime
y In yongJ,nl tlyln银阳极泥提银(extraetion of Silve:fr()nl 511一ver anode slime)见铜阳极泥提金银
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条