1) Zinc phosphate cement
磷酸锌水门汀
1.
Experimental study on shear bond strength of nano composite zinc phosphate cement for prosthodontics
口腔修复用纳米复合磷酸锌水门汀粘接强度的实验研究
2) polycarboxylate cement
聚羧酸锌水门汀
1.
Objective:The aim of this study was to evaluate the effect of different grit sizes of diamond burs on the shear bond strength between prepared dentin and polycarboxylate cement.
目的:比较不同粒度金刚砂车针预备的牙面与聚羧酸锌水门汀的粘固强度。
3) calcium phosphate cement
磷酸钙骨水门汀
1.
Experimental study of effusion in repairing perforation of pulp bottom with calcium phosphate cement;
磷酸钙骨水门汀修复髓室底穿孔后渗漏的实验研究
4) Property improvement calcium phosphate cement
改性磷酸钙骨水门汀
5) eugenol/zinc oxide cement
丁香油氧化锌水门汀
6) Cements
水门汀
1.
Effects of three desensitizers on bonding strength of different cements;
三种脱敏剂对不同水门汀粘接强度的影响
2.
Effects of BisBlock~(TM) desensitizer used on basement tooth on shearing strength of cements.;
牙预备体用BisBlock~(TM)脱敏对水门汀剪切强度的影响
3.
Effect of the Desensitizers Using on Abutment Tooth of the Fixed Dental Prosthetic Restoration on the Bonding Performance of Cements;
固定修复中脱敏剂对水门汀粘接性能影响的实验研究
补充资料:磷酸锌水门汀
分子式:
CAS号:
性质:又称磷酸锌黏固粉。由氧化锌、氧化镁、二氧化硅等粉末和正磷酸、水与氧化铝等液体调制而成。常用作窝洞垫底、暂时充填,黏着嵌体、冠桥、桩冠、甲冠,做根管充填材料等。调制时,将粉与液各适量,分两处放于玻璃板上,用不锈钢调和刀将粉末逐渐加入液内,旋转调合约1~2min即成,立即使用。
CAS号:
性质:又称磷酸锌黏固粉。由氧化锌、氧化镁、二氧化硅等粉末和正磷酸、水与氧化铝等液体调制而成。常用作窝洞垫底、暂时充填,黏着嵌体、冠桥、桩冠、甲冠,做根管充填材料等。调制时,将粉与液各适量,分两处放于玻璃板上,用不锈钢调和刀将粉末逐渐加入液内,旋转调合约1~2min即成,立即使用。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条