1) Two-component Ambient-cured Waterborne Epoxy Resin Coatings
双组分室温固化
2) room temperature cured two-can coatings
室温固化双组分涂料
4) RTV silicone rubber (two components)
室温硫化硅橡胶(双组分)
5) Room temperature curing
室温固化
1.
Study on new two-component room temperature curing acrylate adhesive;
新型室温固化双组分胶粘剂的研究
2.
aration of Room Temperature Curing Bicomponent PU Pouring Sealant;
室温固化双组分聚氨酯灌封胶的制备
3.
Study on synthesis and performance of flexible curing agent for room temperature curing epoxy resin adhesive;
环氧树脂室温固化用柔性固化剂的制备与性能研究
6) curing at room temperature
室温固化
1.
Heat-resistant modification epoxy construction adhesive curing at room temperature;
聚硫醚改性环氧树脂室温固化耐高温结构胶粘剂
2.
Study on high properties adhesive with curing at room temperature;
室温固化高性能胶粘剂的研制
3.
In order to improve the brittleness of epoxy resin after curing,a waterborne epoxy curing agent with toughness curing at room temperature was synthesized.
拟合成一种室温固化柔韧性水性环氧固化剂。
补充资料:双组分室温硫化硅橡胶
分子式:
CAS号:
性质:由羟基封端的二甲基聚硅氧烷以及正硅酸乙酯或聚硅酸乙酯两个组分组成[HO-(Si-(CH3)2-O)n]和(RO)4Si-H硫化前为无色透明到乳白色黏稠流体。硫化胶的硬度(邵氏A)20~70,拉伸强度0.39-2.94MPa或更高,相对伸长率100%~500%。具有优良的介电性能和耐寒、耐热、耐水、耐气候老化等性能,可在-60~+200℃下长期工作。可由羟基封端的二甲基聚硅氧烷、正硅酸乙酯、有机金属羧酸盐催化剂、补强填料等配合混炼而成。使用前,含补强填料的基础胶料以及正硅酸乙酯交联剂和催化剂分别包装成两个组分。使用时混合均匀即可硫化。广泛用于工艺美术品和文物复制的模具胶,也可用作绝缘、防震、密封、灌注、涂覆、嵌缝和粘接等材料。
CAS号:
性质:由羟基封端的二甲基聚硅氧烷以及正硅酸乙酯或聚硅酸乙酯两个组分组成[HO-(Si-(CH3)2-O)n]和(RO)4Si-H硫化前为无色透明到乳白色黏稠流体。硫化胶的硬度(邵氏A)20~70,拉伸强度0.39-2.94MPa或更高,相对伸长率100%~500%。具有优良的介电性能和耐寒、耐热、耐水、耐气候老化等性能,可在-60~+200℃下长期工作。可由羟基封端的二甲基聚硅氧烷、正硅酸乙酯、有机金属羧酸盐催化剂、补强填料等配合混炼而成。使用前,含补强填料的基础胶料以及正硅酸乙酯交联剂和催化剂分别包装成两个组分。使用时混合均匀即可硫化。广泛用于工艺美术品和文物复制的模具胶,也可用作绝缘、防震、密封、灌注、涂覆、嵌缝和粘接等材料。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。