2) cored wires
粉芯丝材
1.
To solve this problem,two kinds of cored wires,Fe-Cr course and Al course,for thermal spray were made,and with arc wire spray technique,intermetallic matrix conposite coatings were got.
为解决此问题,本文设计了两种体系的金属粉芯丝材—Fe-Cr系和Al系,通过电弧喷涂技术制备复合涂层,以解决石油、化工设备中的硫化氢应力腐蚀问题。
2.
The application of the amorphous cored wires for the CFBB has been described in the final of the article.
本文通过介绍循环流化床锅炉的研究背景和失效形式,进而对非晶态涂层的相关结构和性能进行了研究,并在此基础上进一步叙述这种高耐磨粉芯丝材的工业应用。
3.
Fe-based / Cr3C2 composite coatings were prepared using cored wires and high velocity arc spraying (HVAS) technology.
采用高速电弧喷涂技术将自制的铁基Cr3C2型粉芯丝材制备成复合涂层,并对涂层的组织结构、力学性能及高温冲蚀磨损特性进行了研究。
3) magnetic powder core
磁粉芯
1.
Magnetic properties of soft magnetic powder core of nanocrystalline Fe_(73)Cu_1Nb_(1.5)Mo_2Si_(13.5)B_9 alloy;
Fe_(73)Cu_1Nb_(1.5)Mo_2Si_(13.5)B_9纳米晶软磁粉芯磁性能研究
2.
Preparation and soft magnetic properties of composite magnetic powder cores of FeSiB and ferrite
Fe_(78)Si_(13)B_9/铁氧体复合材料磁粉芯制备及其软磁性能
3.
The magnetic powder core was manufactured using 2Mo81Ni17Fe atomized powder and.
本文以氮气雾化2Mo81Ni17Fe合金粉末为原料,采用粉末冶金方法制备了2Mo81Ni17Fe磁粉芯,测试了磁粉芯的磁导率。
4) cored wire
粉芯丝材
1.
Iron-based composite coatings were deposited on mild steel substrate by arc spraying cored wire with WC-CoNi ceramic powders.
采用电弧喷涂含WC-CoNi金属陶瓷粉末的粉芯丝材,在低碳钢基体上制备铁基复合涂层,采用MLS-225型湿砂橡胶轮磨损试验机评价铁基复合涂层的耐磨粒磨损性能,利用光学显微镜、扫描电子显微镜和X射线衍射仪对涂层的显微组织结构、磨损表面及其相组成进行分析。
2.
Three different cored wires holding the WC,TiC or Cr3C2 ceramic powders respectively were fabricated using 304 stainless steel sheath,ferrite-based composite coatings were deposited on the Q235 steel substrate by arc spraying.
分别将WC、TiC、Cr3C2等碳化物陶瓷粉末与304不锈钢带轧制成3种粉芯丝材,采用电弧喷涂技术在Q235钢基体上制备铁基复合涂层。
3.
Development processes of FeCrNi/CBN cored wires were introduced, High velocity arc spraying technology was successfully used to prepare the FeCrNi/CBN coating on 45 steel.
介绍了FeCrNi/CBN粉芯丝材的研制过程,采用高速电弧喷涂技术将所研制的FeCrNi/CBN粉芯丝材成功地在45钢基体上制备出FeCrNi/CBN复合涂层。
5) powder core
磁粉芯
1.
Magnetic properties of amorphous Fe_(74)Al_4Sn_2P_(10) C_2B_4Si_4 powder prepared by water atomization and powder core made from it;
水雾化制备Fe_(74)Al_4Sn_2P_(10)C_2B_4Si_4非晶合金粉末及其磁粉芯性能研究
2.
The powder between 45 μm and 75 μm was used for preparing powder core.
用粒度45~75μm的水雾化粉末制备的磁粉芯具有优异的磁性能,磁导率大于60,良好的频率特性、高的品质因数和低的损耗。
6) cored wire
粉芯线材
1.
Al-based coating is prepared by arc spraying using Al-based cored wire.
采用铝带制作粉芯线材,电弧喷涂方法制备铝基涂层。
补充资料:Z8612热芯盒射芯机操作规程
1、遵守铸造设备通用操作规程。
2、工作前还必须遵守:
a、
检查设备上行程开关和碰块的位置是否正确,如不正确,必须调整。
b、
接通电源,打开压缩空气伐门,先用手动方法,对各机构逐进行点动试车,然后用自动方法,进行一个循环试车,确认一切正常后,方可进行生产。
3、工作中还必须遵守:
a、
在设备开动后,一个循环未完成时,不许中途调整电器,以免发生误动作,造成设备人身事故;
b、
设备的每一个循环后,必须用喷咀清除芯盒上残存的砂子,并喷涂分型剂;
c、
在未切断电源和所气源前,不准将手伸入芯盒和夹紧器之间的空隙处,或把手放在导轨上,以免发生人身事故。
d、 一般不准空射,如必须空射,一定要把压缩空气伐门关小;
e、 如果用手操作,不准同时操作两个电器开关。
4、工作后还必须遵守:
a、
操纵各个电器开关,使设备各机构恢复到原始位置,然后切断电源和气源;
b、 折下射砂头,清理积砂和粘砂;
c、 清除排气塞内的粘砂;
d、
取下射砂筒,清除缝隙中的粘砂,最后用石蜡涂擦内壁,但不要将缝隙堵塞;
e、 清除闸板上的积砂,并在闸板上涂石墨粉,以减少磨擦;
f、 清除导轨和导杆上的积灰和积砂,并涂上一层润滑油。
2、工作前还必须遵守:
a、
检查设备上行程开关和碰块的位置是否正确,如不正确,必须调整。
b、
接通电源,打开压缩空气伐门,先用手动方法,对各机构逐进行点动试车,然后用自动方法,进行一个循环试车,确认一切正常后,方可进行生产。
3、工作中还必须遵守:
a、
在设备开动后,一个循环未完成时,不许中途调整电器,以免发生误动作,造成设备人身事故;
b、
设备的每一个循环后,必须用喷咀清除芯盒上残存的砂子,并喷涂分型剂;
c、
在未切断电源和所气源前,不准将手伸入芯盒和夹紧器之间的空隙处,或把手放在导轨上,以免发生人身事故。
d、 一般不准空射,如必须空射,一定要把压缩空气伐门关小;
e、 如果用手操作,不准同时操作两个电器开关。
4、工作后还必须遵守:
a、
操纵各个电器开关,使设备各机构恢复到原始位置,然后切断电源和气源;
b、 折下射砂头,清理积砂和粘砂;
c、 清除排气塞内的粘砂;
d、
取下射砂筒,清除缝隙中的粘砂,最后用石蜡涂擦内壁,但不要将缝隙堵塞;
e、 清除闸板上的积砂,并在闸板上涂石墨粉,以减少磨擦;
f、 清除导轨和导杆上的积灰和积砂,并涂上一层润滑油。