MCM-22 zeolite, self-support monolithic MCM-22 zeolite have been synthesized by vapor-phase transport method(VPT) and MCM-22/metal support monolithic zeolite has been synthesized by hydrothermal method(HTS) in this study.
本文采用气相转移法(VPT)合成了MCM-22沸石、自支撑整体式MCM-22沸石,水热原位晶化法制备了MCM-22/金属基整体式沸石。
3) MCM-22 zeolite
MCM-22沸石
1.
Ethylbenzene synthesis by catalytic distillation of dry gas and benzene was researched with MCM-22 zeolite as catalyst.
研究了MCM-22沸石催化剂对于干气和苯催化蒸馏制乙苯的反应性能,对β,Y,MCM-22沸石催化剂在催化蒸馏和固定床反应工艺中的催化性能进行了比较。
2.
MCM-22 zeolite was synthesized with hexamethyleneimine as the organic template by hydrothermal synthesis method and was characterized by XRD.
以六亚甲基亚胺为模板剂,采用动态晶化水热法合成了MCM-22沸石,并对其进行了物相表征。
4) MCM-22 zeolite membrane
MCM-22沸石膜
1.
The MCM-22 zeolite membrane was synthesized on an iron-chromium-aluminum alloy foil by the hydrothermal method and characterized by X-ray diffraction and scanning electron microscopy.
采用水热法在铁铬铝合金片载体上原位合成了MCM-22沸石膜,并采用X射线衍射和扫描电子显微镜对沸石膜进行了表征,探讨了成膜的影响因素。
补充资料:整体锻造式高压容器
分子式:
CAS号:
性质:这是用整体锻造炮筒的技术来制造的高压容器,筒体与法兰可整锻而出或用螺纹连接。锻造容器的质量较好,特别适合于焊接性能较差的高强钢所制造的超高压容器。锻造式高压容器一般直径为φ300~φ800,长度不超过12m。在锻造的筒节上也可采用焊接的方法将筒节与筒节、筒节与端部法兰或底部连接起来而组成的容器为锻焊式容器。
CAS号:
性质:这是用整体锻造炮筒的技术来制造的高压容器,筒体与法兰可整锻而出或用螺纹连接。锻造容器的质量较好,特别适合于焊接性能较差的高强钢所制造的超高压容器。锻造式高压容器一般直径为φ300~φ800,长度不超过12m。在锻造的筒节上也可采用焊接的方法将筒节与筒节、筒节与端部法兰或底部连接起来而组成的容器为锻焊式容器。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条