1) erosion/corrosion
冲蚀/腐蚀
2) erosion-corrosion
冲蚀腐蚀
3) erosion corrosion
冲刷腐蚀
1.
The results showed that uniform corrosion,pitting,erosion corrosion and their interaction are the main causes of the failure of the PTA oxidation equipments in the environment containing acetic acid,Br~- and fluid steam and liquid.
结果表明,氧化设备发生的腐蚀失效是由于其在醋酸、Br-、流动的汽/液腐蚀环境下发生了均匀腐蚀、点蚀、冲刷腐蚀和汽蚀以及他们的交互作用所致。
2.
The heating tubes in the 1st section mainly suffer from corrosion of dissolved oxygen while those in the 2nd section suffer from erosion corrosion of high-temperature steam.
其中第一、二节热器管内主要为溶解氧腐蚀 ,而盘管内主要为高温蒸汽的冲刷腐蚀。
4) erosion-corrosion
冲刷腐蚀
1.
Study on Erosion-Corrosion Behavior of Stainless Steel in Acidic Liquid-Solid Two-phase Flow;
酸性液固两相流中不锈钢冲刷腐蚀行为的研究
2.
In Field Electrochemical Detection and Erosion-corrosion Investigation of Metallic Materials in Marine Environment;
海洋环境中金属材料现场电化学检测及冲刷腐蚀研究
3.
The influences of tungsten and carbon content on microstructure,hardness,impact toughness and erosion-corrosion resistance of these cast irons were investigated by metalloscope,image analyzer,X-ray diffraction,electron probe analyzer,mechanical properties test and low angle erosion-corrosion test in salt water sand slurry in this paper.
通过金相组织观察、X射线衍射相结构分析、图像分析仪定量金相测试、电子探针微区成分分析、力学性能检测和盐水砂浆中的低角度冲刷腐蚀试验,研究了含碳量和含钼量对高铬钼钨耐磨铸铁组织、结构、硬度、冲击韧性和抗冲刷腐蚀性能的影响规律。
5) erosion
[英][i'rəuʒən] [美][ɪ'roʒən]
冲刷腐蚀
1.
Using selfmade simulation test stand for copper tubes in condenser of turbines,simulated test of tube erosion for NiP and NiW plated coating and brass HSn 701A has been carried out.
利用自制的汽轮机凝汽器铜管模拟试验装置,进行Ni P、Ni W镀层与黄铜HSn70 1A模拟管端冲刷腐蚀试验。
2.
The resistance to erosion and cavitation-abrasion of the two steels were evaluated by mass-loss method,and corrosion surface morphologies were observed by SEM.
5%NaCl溶液中的冲刷腐蚀和磨蚀性能分别进行测试,用失重法评价了2种材料的抗冲刷腐蚀和磨蚀性能,并利用扫描电镜观察了其腐蚀形貌。
3.
With the self-made erosion test device,the erosion test of HSn70-1A brass and HA177-2A brass was carried out,and the right experiment data were matched into curves.
利用自制的冲刷腐蚀装置,对HSn70-1A、HA177-2A黄铜管进行冲刷试验,对实验数据进行曲线拟合。
补充资料:铂改性铝涂层IN738LC耐蚀高温合金热腐蚀产物