3) anodic aluminum oxide film
阳极氧化铝膜
1.
Growth kinetics and morphological structure of porous anodic aluminum oxide films formed in oxalic acid;
草酸中多孔阳极氧化铝膜生长动力学和形态结构研究(英文)
2.
The preparation technology and morphology analyses of anodic aluminum oxide films containing nanopore arrays on high purity aluminum foils by anodization are reported.
报道了用阳极氧化法在高纯铝片上制备含有纳米孔阵列的阳极氧化铝膜技术,并用原子力显微镜(AFM)和扫描电子显微镜(SEM)对样品形貌进行了分析。
4) aluminum anode oxide film
铝阳极氧化膜
1.
Effects of different sealing hole methods on properties of corrosion resistance of aluminum anode oxide film;
铝阳极氧化膜不同封孔方法的耐腐蚀性能研究
5) anodic alumina membrane
阳极氧化铝膜
1.
Preparation and characterization of a new type of anodic alumina membrane supported by aluminum;
以铝为支撑体的一种新型阳极氧化铝膜的制备与表征
2.
One-step preparation and morphology characterization of anodic alumina membrane with nanopore arrays in oxalic acid solution;
草酸中纳米孔阵列阳极氧化铝膜的一步法制备及其形貌表征
3.
Reasearch on a New Type of Anodic Alumina Membrane Supported by Aluminum;
以铝为支撑体的新型阳极氧化铝膜的研究
6) Anodized aluminum
铝阳极氧化膜
1.
The advance of sealing process on anodized aluminum;
铝阳极氧化膜封孔技术之进展
补充资料:铝的阳极氧化
在酸性电解液中,以铝为阳极,经过电解使铝表面产生氧化膜的材料保护技术。铝的阳极氧化有多种电解液,但基本上是以硫酸、铬酸、乙二酸或硼酸为主要组分配制的。其中最常用的是硫酸基的。电源可采用直流、交流或交变直流的。电压在 5~25伏间,温度低于25℃。电解过程中,氧的阴离子与铝作用产生氧化膜。这种膜初形成时还不够细密,有一定的电阻,使电解液中的负氧离子仍能到达铝表面继续形成氧化膜。随着膜厚度的增长,电阻变大,电解电流变小,而与电解液接触的外层氧化膜同时发生化学溶解,在铝表面形成氧化物的速度渐与化学溶解的速度平衡时,这一氧化膜便可达到这一电解参数下的最大厚度。铝的阳极氧化膜的结构与其他转化膜有所不同,靠近基体金属部分的是0.01~0.1微米的致密层,其上是许多空心六角柱体所构成的蜂房状层,总厚度为2~100微米不等。由各种电解液产生的阳极氧化膜色调不一,有的是整体着色的,多用于建筑工业,有的可以染料着色或利用水解和复分解的方法,使形成的颜料沉积在六角柱的空心部分,增加美感。最后还需要进行封闭和烘干。有阳极氧化铝膜的铝材,抗蚀性有时优于经过铬酸盐处理的铝材。这种铝材除在建筑工业和日用五金产品方面广泛使用外,也用于飞机、汽车、民用船舶。利用低温、溶解力微弱的电解液和较高的电压(100~150伏),可形成工程用的硬质阳极氧化膜,用于与纤维、纸张和橡胶接触的机械零件和液压元件。在普通阳极氧化铝层的六角柱体空洞中填充聚四氟乙烯,可以获得摩擦系数极低的零件。