This paper investigates the effect of binders including calcium aluminate cement,α-Al2O3,calcium aluminate cement with silicon,and α-Al2O3 with silicon on the properties of Al2O3-SiC-C castable.
研究了铝酸钙水泥、铝酸钙水泥/SiO2微粉、-αAl2O3微粉以及-αAl2O3微粉/SiO2微粉4种结合剂对Al2O3-SiC-C质浇注料性能的影响。
3)  Al 2 O 3-SiC-C
Al2O3-SiC-C
4)  Al2O3-SiC-C brick
Al2O3-SiC-C砖
1.
It's proposed that,the Al2O3-SiC-C brick adhibits the molted slag due to the carbon oxidation and the big pores in the brick,while the andalusite-Al2O3-SiC brick does not adhibit the molten slag because it is free of carbon oxidation and big pores.
以大型混铁车用Al2O3-SiC-C砖和红柱石-氧化铝-SiC砖为对象,研究使用后材料粘渣的过程和原因,提出Al2O3-SiC-C质罐衬砖由于C的氧化和砖本身的气孔较大,使材料容易粘渣。
5)  Alumina-silicon carbide based
Al2O3-SiC质
6)  Alumina-silicon carbide-carbon castables
Al2O3-SiC-C浇注料
补充资料:bioactive glass-ceramic composite reinforced by SiC whisker
分子式:
CAS号:

性质:由碳化硅晶须与生物活性玻璃陶瓷复合而成的生物陶瓷复合材料。高强度、高弹性模量、无毒的碳化硅晶须在陶瓷基材中弥散分布,使材料中的裂纹相对均匀,裂纹扩展发生转向和分支;外力作用下碳化硅晶须拔出时产生的拔出效应,使复合陶瓷的弯曲强度达460MPa,断裂韧性达4.3MPa·m1/2,维伯尔系数高达24.7,标志着它是可承力的生物陶瓷复合材料。