A method of combining AC impedance and weak polarization technology to measure corrosion rate of metals is presented.
提出了交流阻抗和弱极化技术相结合的腐蚀速度测量的方法,并依此研制了CMB-4510腐蚀速度测量仪。
2.
The LR03 alkaline Zn-MnO2 batteries were discharged with constant load, which resulted in weak polarization in both the positive and negative electrodes of the batteries at the same time.
采用恒阻放电的方法使LR03碱锰电池正负极同时产生弱极化,使用铂丝作参比电极和Arbin电池测试仪跟踪记录极化数据及极化曲线。
3.
The results are compared with the dynamic potential scanning results in the weak polarization condition.
利用恒电量仪测定了钢筋混凝土中水灰比及二级粉煤灰含量对钢筋 (45 #钢 )的腐蚀行为的影响 ,并用恒电位仪的弱极化动电位扫描曲线解析结果与之比较 。
5) lead implanted aluminium electrode
弱极化区
1.
The anodic polarization curves of lead implanted aluminium electrodes have been determined in sulfuric acid in weak polarization region at 25℃.
在弱极化区测量了 2 5℃时H2 SO4溶液中离子注入铅的铝电极的阳极极化曲线 。
6) weak dipolarizations
弱双极化
补充资料:弱极化法腐蚀速度测定
分子式:
CAS号:
性质:是利用测定极化曲线上介于线性区和强极化区(塔菲尔区,Tafel area)之间的弱极化区内的电位-电流关系来计算金属腐蚀速度和动力学参数的方法。在腐蚀电位附近±60mV内测定E-I曲线,根据极化曲线方程式,用计算机拟合即可算出腐蚀电流和塔菲尔常数。也可通过数学处理后算出上述全部参数,而且对电极表面状态影响不大。
CAS号:
性质:是利用测定极化曲线上介于线性区和强极化区(塔菲尔区,Tafel area)之间的弱极化区内的电位-电流关系来计算金属腐蚀速度和动力学参数的方法。在腐蚀电位附近±60mV内测定E-I曲线,根据极化曲线方程式,用计算机拟合即可算出腐蚀电流和塔菲尔常数。也可通过数学处理后算出上述全部参数,而且对电极表面状态影响不大。