3) high-temperature corrosion
高温腐蚀
1.
Investigations on outer thermal spraying and inner shot blasting on boiler tube to promote high-temperature corrosion resistance;
采用外壁喷涂与内壁喷丸方法提高锅炉高温受热面管抗高温腐蚀性能的试验
2.
The large amount of vanadium in Orimulsion may cause unexpected problems in the prevention of high-temperature corrosion of furnace.
奥里油中含钒量较多,是锅炉预防高温腐蚀设计中的大难题。
3.
The mechanism of high-temperature corrosion on water-wall of coal-fired boilers in thermal power plants has been briefly presented, and preventive countermeasures being put forward directing against different causes of high-temperature corrosion, the prevention technology of spraying corrosion-resistant metallic coatings onto surface of the water-wall being emphatically narrated.
简要介绍了火电厂燃煤锅炉水冷壁高温腐蚀机理,并针对不同的高温腐蚀原因提出了防护对策。
4) high temperature corrosion
高温腐蚀
1.
Study on high temperature corrosion resistance of FeCrAl and NiCr alloy coating;
FeCrAl和高镍铬合金涂层的抗高温腐蚀性能研究
2.
High Temperature Corrosion of Superheater Tube Materials in Pulverized Coal-Fired Environment;
粉煤燃烧环境中过热器管材的高温腐蚀
3.
Cause analysis of high temperature corrosion and precautionary measures for a 300MW boiler furnace;
燃煤锅炉炉膛高温腐蚀原因及对策
5) corrosion at high temperature
高温腐蚀
1.
This paper represents the mechanism of the water wall tube corrosion at high temperature and the principle of spraying Ni-Cr alloy anticorrosion coat , and introduces the characteristics of the high speed arc spraying and construction technology , at the same time also introduces the method of coat quality inspection.
初步阐述了水冷壁管高温腐蚀的机理及喷涂Ni-Cr合金防腐涂层的原理,介绍了高速电弧喷涂技术的特点、施工工艺,同时也介绍了涂层质量的检测方法。
6) thermophilic digestion
高温腐化
补充资料:高温气冷堆工艺供热
分子式:
CAS号:
性质:高温气冷堆运行温度高,可以供给约950℃左右的高温工艺热,为煤的气化和液化供热。用氦气将煤的加氢气化剂加热,把煤转化成中高热值的煤气,它使煤的加氢气化流程简化。高温气冷堆工艺供热在煤的液化中的作用是使过热蒸汽及甲烷重整产生氢气,再经氢煤法和加氢热溶法使煤液化成类似原油的物质。可使成本下降,节约30%~40%矿物燃料,减少环境污染。
CAS号:
性质:高温气冷堆运行温度高,可以供给约950℃左右的高温工艺热,为煤的气化和液化供热。用氦气将煤的加氢气化剂加热,把煤转化成中高热值的煤气,它使煤的加氢气化流程简化。高温气冷堆工艺供热在煤的液化中的作用是使过热蒸汽及甲烷重整产生氢气,再经氢煤法和加氢热溶法使煤液化成类似原油的物质。可使成本下降,节约30%~40%矿物燃料,减少环境污染。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条