说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 轻质高强微膨胀混凝土
1)  high strength micro-expansive lightweight aggregate concrete
轻质高强微膨胀混凝土
1.
Dynamic analysis of arch bridges strengthened with high strength micro-expansive lightweight aggregate concrete;
轻质高强微膨胀混凝土加固拱桥的动力分析
2)  lightweight light-expansion concrete
轻质微膨胀混凝土
1.
In this paper,lightweight light-expansion concrete is applied to the strengthening of arch bridges.
将自行研究配制的轻质微膨胀混凝土应用于拱肋的加固。
3)  High-Strength Light Weight Concrete
高强轻质混凝土
1.
Discussion on the Control of Segregation of High-Strength Light Weight Concrete;
浅谈控制高强轻质混凝土的分层离析
2.
Research on Application of High-Strength Light Weight Concrete to Highway Beam Bridges;
高强轻质混凝土在公路桥梁上的应用研究
4)  light-weighted and high-strengthed concrete
轻质高强混凝土
1.
An experimental research on light-weighted and high-strengthed concrete of expanded fly ash aggregate
陶粒轻质高强混凝土的试验研究
5)  high-strength micro-expansive concrete filled steel tube
钢管高强膨胀混凝土
6)  superplasticized high-strength expansive concrete
高强流态膨胀混凝土
1.
The results show that the expansion of superplasticized high-strength expansive concrete has its characteristics: autogenous shrinkage occurs in 1 d standard curing, and expansion .
研究表明高强流态膨胀混凝土的膨胀行为有其特殊性:在不加磨细矿渣(blastfurnaceslag,BFS)时,水养1d出现自收缩,整个硬化过程膨胀受到抑制,原因在于高强流态膨胀混凝土较高的强度,特别是较高的早期强度限制了膨胀的发挥,在混凝土内部存在"自约束效应"。
补充资料:高强混凝土
分子式:
CAS号:

性质:具有高强度的混凝土。根据我国混凝土的设计和施工水平,认为强度等级达到或超过C50的混凝土为高强混凝土。高强混凝土的特点是耐久、强度高、变形小,能适应大跨度、重载、高层发展,能承受恶劣的环境条件。主要应用于露天的、遭海水侵蚀的、受高速流体冲刷的或易遭碰撞的工程建筑物。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。