1) sulphoslag
硫酸尾渣
1.
According to the analysis and research on the properties of local calcic clay and waste sulphoslag, batching of body onglazed ceramic tiles is designed by cross experimental design.
对钙质粘土及废弃的硫酸尾渣的性能进行分析研究的基础上,采用正交原理优化设计出釉面砖坯料配方,再配以高强乳 浊釉对其有效遮盖,经生产实际运行,产品指标均达到企业标准要求,为地产原料的研发和废弃尾渣的利用提供了一定 的研究基础。
2) Aluminum sulfate tailings
硫酸铝尾渣
1.
Main minerals in the aluminum sulfate tailings are kaolinite and bochmite AlOOH.
研究表明 ,将经过煅烧处理的硫酸铝尾渣和高效减水剂共同掺入水泥中 ,具有较好的早期和后期增强效
3) acid leachin tailings
酸浸尾渣
4) pyrite cinder
硫酸渣
1.
magnetic-separation Preparation of high quality magnetite concentrate from pyrite cinder by composite pellet reduction-roasting and;
硫酸渣复合球团还原焙烧法制备高品位磁铁精矿
2.
Study on recovering Cu,Zn from pyrite cinder with bioleaching method;
微生物浸出法回收硫酸渣中铜、锌的研究
3.
The experiment and industrial application of recovering iron concentrate from pyrite cinder with vertical magnetic separator with pulsating vibration magnetic field were introduced.
介绍了立式脉冲振动磁场磁选机选别硫酸渣(黑渣)试验及工业生产情况,探讨了硫酸渣利用存在的问题及发展方向。
5) sulfuric acid residue
硫酸渣
1.
Preparation of high purity ferrous sulfate from sulfuric acid residue
硫酸渣制备高纯度硫酸亚铁
2.
Iron trichloride purifying agent was prepared by using the low density Hydrochloric acid(density is approximately 20%-30%) recycled from Zunyi Titanium Factory to react with sulfuric acid residue.
采用遵义钛厂在海绵钛氯化生产中回收的低浓度盐酸(浓度约为20%-30%)与硫酸渣进行反应制备三氯化铁净水剂,实验结果表明采用硫酸渣与低浓度盐酸反应制备三氯化铁净水剂是可行的。
3.
A sulfuric acid residue is used for absorbing the chlorine emissions to make FeCl_3 in the laboratory,acid gas HCl within the chlorine emissions and Fe_2O_3 in the sulfuric acid residue are used for carrying on the counteraction reaction, oxidizability of Cl_2 is used for oxidizing Fe~(2+)in the sulfuric acid residue to Fe~(3+),making it to form product FeCl_3.
在实验室采用硫酸渣矿浆吸收含氯废气制取 FeCl_3,利用含氯废气中的酸性气体 HCl 与硫酸渣中的 Fe_2O_3进行中和反应,同时利用 Cl_2的氧化性将硫酸渣中的亚铁离子氧化成三价铁离子,使之形成产品 FeCl_3。
6) Pyritic slag
硫酸烧渣
1.
The article briefly introduced the technology and the craft of Pyritic slag depuration,discussed the major effect factor in make pre-roasted material of Strontium Ferrite by the depuration,and in the big production the final magnetic performance stably achieve Br:400 mT,Hcb:270 kA/m,Hcj:280 kA/m,(BH)m:32 kJ/m~3.
文章介绍了硫酸烧渣提纯的技术和工艺,探讨了提纯后的原料做锶铁氧体预烧料的主要影响因素,使预烧料生产的锶永磁铁氧体磁性能稳定达到Br:400 mT,Hcb:270 kA/m,Hcj:280 kA/m,(BH)m:32 kJ/m3以上。
2.
Aimed at utilization of iron resources in pyritic slag,the study on production of metallized agglomerate with pyritic slag through coal based DR process was conducted.
为合理利用硫酸烧渣中的铁资源,进行了煤基直接还原生产金属化团块的研究,提出了润磨造球-预热焙烧-磁选-冷固结成型的新工艺流程。
补充资料:干渣渣