1 were prepared by methods of supersonic and co-deposition, Pechini and high temperature solid phase reaction according to substitution of anion-cation combination.
以阴阳离子复合掺杂为基础,采用超声共沉淀法、Pechini法和高温固相法合成尖晶石型掺杂锰酸锂前驱体,使用3段热处理方式,即650℃预烧、780℃烧结、550℃回火制备得到掺杂尖晶石LiCo0。
2) ultrasonic codeposition
超声共沉淀
1.
Fe_3O_4 nanoparticles were prepared with ultrasonic codeposition method.
本文通过超声共沉淀法制备了 Fe_3O_4纳米颗粒。
4) Ultrasonic precipitation
超声沉淀法
5) ultrasonic co-deposition
超声波共沉淀
1.
The SO2-4/Fe2O3-ZrO2 solid superacid(SFZ-n,n=1~12) were prepared by ultrasonic co-deposition and then aged for 24 h at-15 ℃.