说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 最大成形梯度
1)  max forming grads
最大成形梯度
2)  maximum gradient
最大梯度
1.
The definitions of grid data gradient (directional derivative, gradient and maximum gradient) and their application ranges are analysed and discussed, and their analytical calculation formulas and discrete calculation formulas are given.
分析和讨论了关于网格数据梯度的定义(方向导数,梯度,最大梯度)及其应用范围,给出了解析计算公式和离散计算公式。
2.
A simple algorithm for threshold alternative and localization criteria based on maximum gradient is proposed to overcome typical Sobel operater\'s disadvantages of the obtained image edges being thick and causing edge point misjudgement.
针对高能闪光照相中投影图像的特点,对数字图像处理中具有代表性的Sobel边缘检测算法进行了分析,发现该算法存在检测出的边缘粗和人为进行阈值的选取会造成边缘点的误判的缺点;为此提出了一种阈值确定方法和基于最大梯度的定位准则算法。
3)  maximum gradient search method
最大梯度法
4)  maximum gradient difference
最大梯度差
1.
The traditional MGD(maximum gradient difference) algorithm based on the order of the image pixels matrix has the shortcomings of the large operation measure and long-time running.
车牌定位是车牌自动识别系统中关键的第一步,传统的最大梯度差算法按图像像素矩阵的顺序进行扫描和运算,存在运算量大,耗时长的缺点。
5)  maximum of gradients
梯度最大值
6)  maximum gradient
最大梯度,最大坡度
补充资料:主要射出成形材料成形时应注意事项

■主要射出成形材料成形时应注意事项
品  名 注    意    事    项
PVC
聚氯乙烯
1.  产品种类范围非常广(硬质、软质、聚合物等),成型条件各有不同,从熔融至分
解之温度范围很小,尤须注意加热温度。
2. 附着水分少,但成型周期尽可能减少(50℃~60℃热风干燥)。
3. 成型机方面,与材料直接接触的部位须电镀或采用不锈钢以防热分解所产生的盐酸
侵蚀。射出压力2100kg/cm2程度。
4. 所有塑料当中必须是细心注意温度调节。
5. 浇口附近易产生流纹,故射出操作后,柱塞不要后退使浇口充分固化后再瞬间退后为宜。
6. 加热之初温不宜高,特别注意熔融情形。第二级加热温度较高,且尽可能使成形周
期缩短,比较安全。


PA
聚醯胺树脂
1. 成型温度比其它材料高,故采用油加热的成形机较适当。
2. 吸湿性大,必须充分干燥。水分对成型品的品质影响甚大(80℃热风干燥约5~6小时)。
3. 须退火以消除内部歪斜。
PP
聚丙烯
1.  同PE,但成形温度必须较高。熔融温度170℃,超过190℃则流动性大增,则毛边增加,
易产生接缝及凹入情形。


PC
聚碳酸脂
1. 吸湿性比尼龙小,但若有些微之水分存在则成型品产生其它色泽或气泡,故必须密封
干燥同时成形时也须预备干燥(120℃之温度4小时)。
2. 加热温度超过320℃时则产生热分解,成品变色,故特别注意温度调节,又成型时的温度调节也非常重要,须特别注意其最低温度、最低时间。
3. 须退火以消除内部歪斜(130℃~135℃,1小时程度为准)。