1) LiNbO3 integrated optic modulator
铌酸锂集成光学调制器
1.
The characteristics and system test method of the core optical component——the LiNbO3 integrated optic modulator used in high accuracy fiber optic gyros(bias is better than 0.
01(°)/h)中的核心光学器件——铌酸锂集成光学调制器在光纤陀螺中的调制特性及系统测试方法进行了探讨,对其应用及与光路其他各部分配合的技术进行了理论分析和实验研究。
2) LiNbO_3 electro-optic modulator
铌酸锂电光调制器
3) Lithium niobate integrated circuit
铌酸锂集成光路
4) LiNbO_3 modulator
铌酸锂调制器
1.
A kind of ultra-short optical pulse source based on commercial LiNbO_3 modulators is proposed.
提出了一种基于商用化的铌酸锂调制器产生超短光脉冲的方法。
5) LiNbO3 modulator
铌酸锂调制器
1.
A phase and intensity hybrid modulation method using commercial LiNbO3 modulators was developed to reduce the cost of an ultra-short optical pulse source.
为了获得低成本的高重复频率超短光脉冲源,满足高速光时分复用(OTDM)的需求,该文使用商用的铌酸锂调制器对连续光进行相位-强度调制,利用色散补偿光纤(DCF)和梳状色散光纤链(CDPF)对产生的光脉冲分别进行啁啾补偿、非线性压缩。
2.
The output character of the DFB-LD,the character of the FBG filter and the modulation of the LiNbO3 modulator are analyzed.
本文建立了光孤子传输的实验系统,分析了增益开关半导体激光器的输出特性,光纤光栅滤波器的滤波特性及铌酸锂调制器的调制特性。
6) lithium niobate integrated circuit
铌酸锂集成光路<光>
补充资料:铌酸锂晶体
分子式:LiNbO3
CAS号:
性质:无色透明体。三方晶系,钛铁矿(畸变钙钛矿型)结构。熔点1253℃,密度4.648 g/cm3。莫氏硬度5,折射率n0=2.297,ne=2.208(λ=600nm),介电常数ε11=44,为铁电晶体,居里点1210℃。自发极化强度50×10-6C/cm2。以碳酸锂和五氧化二铌为原料,晶体在铂金坩埚中用提拉法生长。为一种具有压电、铁电、电光、非线性光学、热电等多性能材料,在微声技术中用于表面波、体波、换能器元件,激光技术中用于调Q开关。还可作全息记录介质材料。
CAS号:
性质:无色透明体。三方晶系,钛铁矿(畸变钙钛矿型)结构。熔点1253℃,密度4.648 g/cm3。莫氏硬度5,折射率n0=2.297,ne=2.208(λ=600nm),介电常数ε11=44,为铁电晶体,居里点1210℃。自发极化强度50×10-6C/cm2。以碳酸锂和五氧化二铌为原料,晶体在铂金坩埚中用提拉法生长。为一种具有压电、铁电、电光、非线性光学、热电等多性能材料,在微声技术中用于表面波、体波、换能器元件,激光技术中用于调Q开关。还可作全息记录介质材料。