说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 等离子淬火
1)  plasma hardening
等离子淬火
1.
This paper summarizes the characteristics of robot plasma hardening to the against erosion zone,the process tests,the satisfactory results and the production experiences of a lot of parts.
本文概述了机械手等离子淬火工艺的特点、工艺试验及批量生产的优良结果与生产业绩。
2)  plasma arc quenching
等离子弧淬火
1.
The quenching surface appearances,metallography organizations and the lubricating state of friction pair were studied and analyzed through testing the impact of plasma arc quenching surface grid on the friction and wear.
研究了等离子弧淬火表面网格对摩擦磨损性能的影响,对淬火网格表面形貌、金相组织、摩擦副之间的润滑状态等进行了分析。
2.
There are two reprocessed technologies after plasma arc quenching,they are lapped finishing and chemical running-in.
等离子弧淬火后处理工艺主要采用研磨和化学跑合2种方法。
3.
The surface hardening treatment of 40Cr alloy steel slag cam was carried out by laser and plasma arc quenching surface hardening technology.
采用激光和等离子弧淬火表面硬化技术对40Cr合金钢碎渣机凸轮表面进行硬化处理,并对修理后的组织和性能进行了研究。
3)  plasma surface quenching
等离子表面淬火
1.
High hardness on die surface and good strength and toughness in the body can be acquired by plasma surface quenching technique.
本文介绍了常压等离子表面淬火的基本机理、加工系统、工艺特点以及性能特性,并给出了有关工艺参数的选择与应用实例。
2.
It was pointed out that hardening holding time is an important factor in the course of forming hardened layer by plasma surface quenching which belongs to short time quenching.
等离子表面淬火硬化层的硬度分布 ,在某一区域内无明显的硬度梯度 ,这与常规淬火方法的结果不太一样。
4)  plasma surface quench
等离子体表面淬火
1.
The parameters of the plasma surface hardening technology of 45 steel are given the hardness of 45 steel by plasma surface quenching was about HV800,The method of heat treatment by using plasma as heat source was feasible.
利用等离子体作为热源对45钢进行表面淬火,通过试验获得等离子体表面淬火热处理的最佳工艺参数,并分析各种工艺参数对淬硬层硬度、深度的影响规律,从而确定45钢等离子弧表面淬火的工艺参数。
5)  austempering [,ɔ:s'tempəriŋ]
等温淬火
1.
Effects of Si and Austempering on the Wearresistance Property of ZG30SiMnCr;
Si及等温淬火工艺对ZG30SiMnCr耐磨性的影响
2.
Effect of Austempering on Mechanical Properties and Abrasion-Resistance of Mn -Cr Alloyed White Cast Iron;
等温淬火对Mn-Cr白口铸铁力学性能和耐磨性的影响
3.
Research of austempering process of low-carbon ductile iron;
低碳球铁的等温淬火工艺研究
6)  isothermal hardening
等温淬火
1.
Strengthening and Toughening of Die Steel Cr7Mo3V2Si by Isothermal Hardening with Prenitriding and Diffusion;
模具钢Cr7Mo3V2Si渗扩氮等温淬火复合强韧化
2.
The influences of various isothermal hardening treatments on microstructure and properties of semi-steel made by quenching and isothermal hardening and forging,which contain 1.
研究了空淬、等温淬火及锻热等温淬火对含1。
3.
2)=900~1000 MPa,σ_b=1300~1564 MPa)and excellence plasticity(δ_5=15%~18%)were obtained after aus- tenitization at 840~880℃followed by isothermal hardening for 3 hours.
试验用钢经840~880℃加热,保温20min,在320~360℃的盐浴炉中等温淬火3 h,得到较高的强度(σ_(0。
补充资料:淬火裂纹和非淬火裂纹的特征及实例分析

淬火裂纹是指在淬火过程中或在淬火后的室温放置过程中产生的裂纹。后者又叫时效裂纹。造成淬火开裂的原因很多,在分析淬火裂纹时,应根据裂纹特征加以区分。


一、淬火裂纹的特征


在淬火过程中,当淬火产生的巨大应力大于材料本身的强度时,便会导致裂纹产生。淬火裂纹往往是在马氏体转变开始进行后不久产生的,裂纹的分布则没有一定的规律,但一般容易在工件的棱角槽口、截面突变处形成。


在显微镜下观察到的淬火开裂,可能是沿晶开裂,也可能是穿晶开裂;有的呈放射状,也有的呈单独线条状或呈网状。


因在马氏体转变区的冷却过快而引起的淬火裂纹,往往是穿晶分布,而且裂纹较直,周围没有分枝的小裂纹。


因淬火加热温度过高而引起的淬火裂纹,都是沿晶分布,裂纹尾端尖细,并呈现过热特征:结构钢中可观察到粗针状马氏体;工具钢中可观察到共晶或角状碳化物。


表面脱碳的高碳钢工件,淬火后容易形成网状裂纹。这是因为,表面脱碳层在淬火冷却时的体积胀大比未脱碳的心部小,表面材料受心部膨胀的作用而被拉裂呈网状。


二、非淬火裂纹的特征


淬火后发生的裂纹,不一定都是淬火所造成的,一般可根据下面的特征来区分。


淬火后发现的裂纹,如果裂纹两侧有氧化脱碳现象,则可以肯定裂纹在淬火之前就已经存在。淬火冷却过程中,只有当马氏体转变量达到一定数量时,裂纹才有可能形成。与此相对应的温度,大约在250℃以下。在这样的低温下,即使产生了裂纹,裂纹两侧也不会发生脱碳和出现明显氧化。所以,有氧化脱碳现象的裂纹是非淬火裂纹。


如果裂纹在淬火前已经存在,又不与表面相通,这样的内部裂纹虽不会产生氧化脱碳,但裂纹的线条显得柔软,尾端圆秃,也容易与淬火裂纹的线条刚健有力,尾端尖细的特征区别开来。


三、实例分析


实例一:


40Cr钢制成的转子轴,经锻造、淬火后发现裂纹。裂纹两侧有氧化迹象,经金相检验,裂纹两侧存在脱碳层,而且裂纹两侧的铁素体呈较大的柱状晶粒,其晶界与裂纹大致垂直。结论:裂纹是在锻造时形成的非淬火裂纹。


当工件在锻造过程中形成裂纹时,淬火加热即引起裂纹两侧氧化脱碳。随着脱碳过程的进行,裂纹两侧的碳含量降低,铁索体晶粒开始生核。当沿裂纹两侧生核的铁素体晶粒长大到彼此接触后,便向离裂纹两侧较远的基体方向生长。由于裂纹两侧在脱碳过程中碳浓度的下降,也是由裂纹的开口部位向内部发展,因而为铁素体晶粒的不断长大提供了条件,故最终长大为晶界与裂纹相垂直的柱状晶体。


说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条