说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 喷射-沉淀法
1)  spraying-coprecipitation method
喷射-沉淀法
1.
Nanostructured Ni-Zn ferrite was successfully prepared by spraying-coprecipitation method.
采用喷射-沉淀法成功地制备了纳米晶 Ni-Zn 铁氧体粉料。
2)  spraying-coprecipitation method
喷射-共沉淀法
1.
Synthesis and magnetic properties of nanocrystalline CoFe_2O_4 ferrite by using spraying-coprecipitation method;
喷射-共沉淀法合成纳米晶CoFe_2O_4及磁性能
2.
Nanocrystalline Ni1-xZnxFe2O4 ferrite with 0≤x≤1, was successfully prepared by a spraying-coprecipitation method.
采用喷射-共沉淀法制备了纳米晶Ni1-xZnxFe2O4(0≤x≤1。
3)  spraying coprecipitation
喷射共沉淀
1.
Characteristic and preparation of nano gas sensitive materials by spraying coprecipitation;
纳米气体敏感材料的喷射共沉淀法制备及特性
2.
In this paper the coprecipitation were improved (called spraying coprecipitation) to prepare nano oxidematerials.
本文在化学共沉淀法的基础上进行改进,称为喷射共沉淀法,采用此方法制备了一些具有良好形貌纳米氧化物材料,并对喷射共沉淀法原理进行了分析。
4)  precipitation-spray drying
沉淀-喷雾干燥法
1.
Nanocrystalline SiC powder was synthesized by carbothermal reduction of the precur- sor of carbon black and silica gel prepared by precipitation-spray drying slurry of carbon black and water glass.
以廉价的水玻璃和炭黑为原料,采用沉淀-喷雾干燥法制备反应前驱体,经碳热还原合成碳化硅。
5)  liquid-precipitate-microwave
微波辐射沉淀法
1.
Fe2O3 nanoparticles support on modified carbon nanotubes(CNTs) were synthesized by liquid-precipitate-microwave method,and the FeCl3 as iron source.
本文研究了微波辐射沉淀法制备碳纳米管负载Fe2O3粒子。
6)  radioactive precipitation analysis
放射性沉淀法
补充资料:空气喷射变形法
分子式:
CAS号:

性质:化纤长丝生产中变形技术的一种。系指丝条通过一个特殊设计的管段,在空气高速喷射的作用下,空气喷射使丝条分开、弯曲成环圈、局部发生缠联,以使获得变形效果的加工方法。产品被叫作空气变形丝,不具有热塑性的长丝,用该项技术也可进行变形。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条