1) destructive test
破坏试验
1.
This paper presents the destructive test of full sized model for vierendeel sandwich plate.
本文对空腹夹层板足尺节点模型做了破坏试验研究,得到结构受荷变形至破坏的全过程载荷—变形曲线,并与理论分析结果相比较,得到许多有价值的结论。
2.
Through the static load destructive test of three different steel reinforced concrete test beams,the test results of three test beams separately of no-pasted carbon fiber cloth,1-layer pasted carbon fiber cloth and 2-layer pasted carbon cloth are given.
该文通过对三种不同的钢筋混凝土试验梁进行静载破坏试验,分别获得了未贴碳纤维布、贴一层碳纤维布及贴两层碳纤维布三种试验梁的试验结果。
2) destruction test
破坏试验
1.
Condition Verification on Destruction test of Self-healingLow-voltage Shunt Capacitor;
自愈式低电压并联电容器破坏试验条件验证
2.
Finally,a research plan of size effect covering large size of concrete members destruction tests was suggested.
为提高大尺寸钢筋混凝土构件设计的合理性,对各国钢筋混凝土构件的尺寸效应研究现状进行了综述与分析,并重点介绍了混凝土强度、钢筋混凝土梁和钢筋混凝土柱的尺寸效应试验研究成果;在归纳总结的基础上,对钢筋混凝土构件尺寸效应研究的发展进行了展望,建议了进行涵盖大尺寸混凝土构件破坏试验的尺寸效应研究方案。
3) failure test
破坏试验
1.
Based on the former achievements and the known basic dynamic property of fly-ash dam,earthquake response tests of Ⅵ and Ⅶ degrees simulation earthquake waves and failure tests have been done on the models of fly-ash dams with different dam crest elevations of 170,180,230 m by the large-scale shaking table.
以某电厂填顶高程170,180,230 m灰坝的模型为研究对象,基于基本动力特性试验,进行了在有干滩和无干滩两种工况下模拟Ⅵ度与Ⅶ度地震烈度的响应试验和破坏试验研究,同时对用3种不同灰渣拌合料加高的180 m高程灰坝模型进行了抗震性能做出评价。
4) destructive experiment
破坏性试验
1.
The Xinxingtang bridge on Huning expressway was taken as an example for introducing the method of destructive experiment of prestressed concrete continuous box girder bridge.
以沪宁高速公路新兴塘大桥主桥为例,介绍了预应力混凝土连续箱梁桥破坏性试验的方法,对加载方式、测试方法、试验现象和试验终止条件等进行了详细描述。
5) destructive test
破坏性试验
1.
From the destructive test of artificial sill pillars which are made of two different kindsof materials, it shows that the steel fiber reinforced concrete is superior to reinforced concrete and theemployment of steel fiber reinforce concrete would creat a possibility to further decrease the thicknessof sill pillar.
通过两种材料的人工底柱破坏性试验表明,钢纤维钢筋混凝土比钢筋混凝土有更多的优越性,使用钢纤维钢筋混凝土有进一步降低底柱厚度的可能性。
2.
According to the condition of nationalbridgs in China, how to carry on the bridge members destructive test of removed from real bridge is reviewed in details,including experiment content,steps,preparation work,loading course.
根据我国桥梁现状,从试验内容、试验步骤、试验准备、荷载试验流程4个方面详细介绍了进行实桥拆除构件实验室破坏性试验工作,为既有钢筋混凝土桥梁进一步的耐久性研究提供了试验资料,可供同类型试验研究工作参考。
3.
This paper details the plan, preparation, procedures, and loading steps of destructive testing on bridge members removed from actual bridge.
根据我国桥梁现状 ,从试验内容、试验步骤、试验准备、荷载试验流程等 4个方面详细介绍了实桥拆除构件试验室破坏性试验工
6) HBsAg killing test
HBsAg破坏试验
补充资料:橡胶密封圈压缩破坏试验
分子式:
CAS号:
性质:在O形密封圈处于扭转变形状态下,加以相当大的负荷,进行压缩,以检查其有无损坏的试验。O形密封圈在动态使用中的扭转变形是其密封失效的一个主要原因,由本试验可检验在动态下使用的O形圈的抗扭转变形能力。
CAS号: