1) cathodic hydrogen charging
阴极电解充氢
1.
Effect of cathodic hydrogen charging on the ductility of steel 1Cr18Ni9Ti was investigated by means of repeated bend test.
本文采用阴极电解充氢和反复弯曲试验方法,考察了氢对1Cr18Ni9Ti钢的塑性变形能力的影响。
2) electric hydrogen-charging
阴极充氢
1.
The results show that the hydrogen penetrated into the sample after the electric hydrogen-charging aggregated into bubbles in the fusion zone.
利用阴极充氢法研究了堆焊熔合区裂纹形核机理。
3) electrolysis-cathode-hydrogenating
阴极电解渗氢
1.
The effect of plastic deformation on the solution and escape of hydrogen in low-carbon steel has been investigated by using electrolysis-cathode-hydrogenating method the solution hydrogen can not larger the solution diffusivity and the smaller the escape diffuivity .
用阴极电解渗氢法研究了塑性变形对低碳钢中溶氢和逸氢过程的影响。
4) electrochemical hydrogen charging
电解充氢
1.
A technique of electrochemical hydrogen charging was used to study the behavior of hydrogen-induced cracking.
采用电解充氢方法对2。
2.
A technique of electrochemical hydrogen charging is introduced in this paper to study the hydrogen embrittlement of 21/4Cr1Mo hydrogenation reactor steel.
用电解充氢方法研究了加氢反应器用2-1/4Cr-1Mo钢的氢脆。
3.
A technique of electrochemical hydrogen charging is adopted to study the behavior of hydrogen-induced cracking of 2.
采用电解充氢方法分别对回火脆态和脱脆态2。
5) electrolytic hydrogen charging
电解充氢
1.
The factors influencing hydrogen-induced disbonding were studied through a series of electrolytic hydrogen charging tests.
通过电解充氢试验研究了不锈钢堆焊层剥离断裂的影响因素,并着重分析了这一断裂问题的金属学本质。
2.
The factors influencing hydrogen-induced disbonding are studied through a series of electrolytic hydrogen charging tests, and the finite element method are adopted for computing the distribution of hydrogen concentration in weld overlay structures.
通过一系列电解充氢试验研究了堆焊层剥离的影响因素,并采用有限元分析方法计算了堆焊结构中氢浓度的分布。
3.
The basis,theory and equipment of the electrolytic hydrogen charging test are discussed in detail.
本文对电解充氢法用于不锈钢堆焊层氢致剥离研究的试验依据、原理和试验装置作了详尽的叙述,从试验和理论计算两方面与传统方法进行了比较。
6) cathodic electrolysis
阴极电解
1.
Cerium-rich conversion coatings were deposited on porous film of anodized auminoum by cathodic electrolysis in a solution containing 1 g/L CeCl 3·7H 2O and 10 ml/L H 2O 2.
通过阴极电解的方法在铝合金多孔阳极氧化膜上沉积了富铈转化膜 。
2.
Electrochemical measurements, corrosion tests, SEM and EDAX were used to investigate forming cerium conversion coatings on aluminum alloys in cerium salt solutions by cathodic electrolysis.
在铈盐溶液中用阴极电解的方法沉积铝合金铈转化膜,用电化学测试、腐蚀实验、SEM和EDAX等分析手段研究了转化膜的性能。
补充资料:年产电锌10万t电解车间采用1.6m~(2)大阴极电解槽