1.
The cyclic plasma oxynitriding test of 0Cr18Ni9 austenitic stainless steel had been performed and compared with conventional ion nitriding processing.
对0Cr18Ni9奥氏体不锈钢进行氮氧共渗循环离子渗氮试验,并和常规离子渗氮进行对比。
3)  austenite stainless steel 0Cr18N i9
奥氏体不锈钢0Cr18Ni9
4)  austenite steel
奥氏体钢
1.
The interface lattice misfitting theory can not explain that TiC and CaS act as an efficient catalyzer during the non-equilibrium solidification of austenite steel.
利用界面共格对应理论无法解释奥氏体钢非平衡凝固过程中TiC、CaS为奥氏体枝晶有效异质核心的现象。
2.
The performance of granular γ+(Fe,Mn)3C eutectics reinforced austenite steel matrix composites (EAMC) was studied, and the strengthening/toughness match and wear resistance were analyzed.
在研究团球γ+(Fe,Mn)3C共晶体增强奥氏体钢基自生复合材料(EAMC)的力学与耐磨性能的基础上,分析了EAMC的强韧化及耐磨机理。
3.
The effect of sliding velocity on the friction behaviors of in situ granular 7+(Fe, Mn)3C eutectics reinforced austenite steel matrix composites (EAMC) has been investigated by the pin-on disc dry sliding tests and scanning electron microscopy (SEM) observation.
利用MPX-2000型主轴盘销式磨损实验机和扫描电子显微镜(SEM)研究了相对滑动速度对团球γ+(Fe,Mn)_3C共晶体增强奥氏体钢基自生复合材料(EAMC)摩擦学性能的影响。
5)  austenitic steel
奥氏体钢
1.
The direct relationship between stacking fault energy and phase transformation driving force of austenitic steels and the effect of stacking fault energy and strain energy on the morphology of martensite are deduced.
导出了在奥氏体钢中相变驱动力与层错能的关系以及层错能和应变能对马氏体形态的影响规律。
2.
The effects of stacking fault energy and strength on phase transformation in cryogenic austenitic steels were studied.
研究了低温奥氏体钢中层错能和强度对相变的作用 ,导出了相变临界分切应力和层错能与强度之间的关系式。
6)  austenitic steels
奥氏体钢
1.
On the basis of systematical study,the comprehensive effects of alloying elements in cryogenic austenitic steels were analyzed.
在系统研究结果的基础上,分析总结了低温奥氏体钢中合金元素的综合作用。
2.
The recent developments of cryogenic austenitic steels are reviewed.
综述了低温奥氏体钢的研究进展 论述了高锰、高氮奥氏体钢低温脆断模式及其断裂机理 ,指出不同合金化的高锰、高氮奥氏体钢有着不同的层错能、相变临界分切应力、解理强度、屈服强度 ,因而有不同的断裂现象 ,包括晶间开裂、穿晶脆断、退火孪晶界开裂 着重探讨了穿晶脆断现象 ,指出穿晶脆断是高锰含氮奥氏体钢特有的脆性断裂形式 提出了今后的研究方