1)  masking
掩蔽保护
1.
The basic items on masking PSA tapes for various processes are described briefly.
在简单涉及有关加工工艺用保护性压敏胶粘带的一些基本概念的基础上 ,着重探讨了基材、压敏胶主体材料、添加剂、交联等对胶粘带掩蔽保护效果的影响。
2)  Masking
掩蔽
1.
Discussion on the Masking and Demasking Problem in Analytical Chemistry Teaching Materials of Pharmaceutical Engineering;
关于制药工程专业分析化学课程教学中掩蔽与解蔽问题的讨论
2.
A Reseach on Masking Method for S~(2-) in Basicity Determination of OH~- CO_3~(2-) and HCO_3~-;
OH~-、CO_3~(2-)和HCO_3~-碱度测定中S~(2-)的掩蔽方法研究
3.
A Diagnosis of Cochlear Hydrops Using ABR under Masking of Pink Noise;
粉红噪声掩蔽下的听性脑干反应诊断早期梅尼埃病
3)  shelter
掩蔽
1.
By means of sheltering the chief reductive substances in the total drain sludge one by one and analyzing the changes of COD before and after the shelters,the writer finds out the primary factors which influence the COD.
通过对总排污口污水中主要还原性物质逐项进行掩蔽 ,分析掩蔽前后污水COD值的变化 ,找出了影响COD的主要因素并提出了改进措施 ,使排污总口COD值大幅降
2.
The function of sheltering nitrite from sulfamic acid is compared with that from sodium azidum.
结果表明:海洋监测规范中COD的测定方法不适合于NO-2较高的污染海水,比较了氨基磺酸与叠氮化钠对NO-2的掩蔽效果及测定方法。
3.
And adopt active carbon pretreatment,EDTA complexing,NH_4F shelter and pH control resolve these unstabilizing factors.
采取了活性炭预处理、乙二胺四乙酸钠络合、氟化铵掩蔽和酸度控制等方法来解决不稳定性,并且与火法试金分析结果进行对照,结果相符,方法可行。
4)  masking agent
掩蔽剂
1.
To find out a method which not only shorten time,save money and decrease pollution,but also satisfy requirements for setting out chemical oxygen demand(COD),the CODs were quickly determined by mercury-free potassium dichromate method using MnSO4 as catalyst and AgNO3,KCr(SO4)2·12H2O as masking agent of Cl-in sulfuric-phosphoric mixed acid.
12H2O作Cl-的掩蔽剂,采用重铬酸钾氧化法,无汞快速测定COD。
2.
In this method the masking agent is directly introduced into the determination to eliminate the interference of interfereing elements.
直接加入掩蔽剂消除铅测定中干扰元素对铅的干扰,用此方法对铅铋合金中的铅进行了准确的测定,取得了很好的准确度和重现性。
3.
The pH of both the beginning precipitation and the completion of precipitation,of the slightly soluble compounds,can be determined very conveniently through the logα M(L) -pH curve masking diagram under the conditions of the existence of masking agent.
本文提出的图解法 ,可极为简便地确定掩蔽剂存在时微溶物开始沉淀及沉淀完全时的pH值 ,比文献[1~ 3 ] 方法易于求解 ,计算简便。
5)  Sb and Bi
掩蔽方法
6)  masking action
掩蔽作用
参考词条
补充资料:材料保护 :电化学保护
    通过改变极性或移动金属的阳极极化电位达到钝态区来抑制或降低金属结构腐蚀的材料保护技术。从伽法尼电池的两个金属电极来观察﹐腐蚀总是发生在阳极上。阴极保护就是在潮湿的土壤或含有电解质(如盐等)的水液等电解液中﹐利用牺牲阳极(如锌﹑铝等)或外加电流的惰性阳极﹐使被保护的钢铁结构成为这种人为的伽法尼电池中的阴极。在同一腐蚀环境中﹐活性较大的是阳极﹐较小的是阴极﹐例如在海水中﹐锌与低碳钢间如构成电解电池﹐锌就是阳极﹐钢就是阴极﹔但如果钢与不锈钢形成电解电池时﹐钢又变为阳极﹐不锈钢是阴极。所谓阴极﹐实际上是使电解液中的阳离子获得电子而还原的一个电极。因此﹐利用外加直流电源使它获得电子补充﹐也属於阴极保护方法。在不同的腐蚀介质中所需的保护电流密度不一。钢在土壤内﹐约为 0.0001~0.005安/分米3﹐在流动海水中约为0.0003~0.0015安/分米3﹐而在流动淡水中为0.005安/分米3 。阴极保护广泛用於保护地下管道﹑通信或电力电缆﹑闸门﹑船舶和海上平台等以及与土壤或海水等接触面积很大的工件﹐电化学保护与涂装结合则更为经济。城市和大型工厂的地下金属设备可採用这种保护方法﹐但需要注意杂散电流不致影响邻近地下金属设施的加速腐蚀。阳极保护主要用於保护钢﹑不锈钢和鈦等在浓硫酸和磷酸等强介质中的腐蚀。活性-钝性金属在阳极极化时﹐即电流导入而產生电位变化时﹐其极化曲线中有显著的活化﹑钝化和过钝化区(见图 阳极保护原理的极化曲线 )﹐对於这种情况﹐可利用稳压电源将电位控制在钝化区间﹐使腐蚀电流值降到最低限度。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。