说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 20CrMnTi钢接头组织
1)  structure of 20CrMnTi steel joint
20CrMnTi钢接头组织
2)  20CrMnTi steel
20CrMnTi钢
1.
Determination of dislocation densities and crystal structure on 20CrMnTi steel;
20CrMnTi钢的位错密度及晶体结构
2.
Influence of forming temperature on flow characteristics of carburized 20CrMnTi steel;
20CrMnTi钢渗碳后变形温度对流变特性的影响
3.
Tooth fracture failure analysis of carburized 20CrMnTi steel gear
20CrMnTi钢渗碳齿轮断齿失效分析
3)  joint microstructures
接头组织
4)  microstructure [英]['maikrəu,strʌktʃə]  [美]['maɪkro,strʌktʃɚ]
接头组织
5)  joint microstructure
接头组织
1.
The joint microstructure is fine and homogeneous,and some welding defects such as crack and blowholes .
3N奥氏体钢TIG焊接接头的组织及低温力学性能 ,结果表明 ,采用氮 -氩混合气体保护的TIG焊接方法可获得满意的接头组织和性能。
2.
According to the analysis of nucleation size and joint microstructure,the welding machine and performance is stable,the welding quality of the welding joint is good when the voltage is 110 V and the pressure is about 15 N.
通过对熔核尺寸和接头组织的分析,结果表明:该焊机性能稳定;当电压为110V、压力为15N左右时,能够得到质量较好的焊接接头。
3.
The process,joint microstructure,mechanical property and influencing factors of LFW were mainly introduced and the research status and application of LFW both home and abroad were summarized.
本文主要介绍了线性摩擦焊的工艺过程、接头组织、力学性能以及各种影响因素,最后综述了线性摩擦焊在国内外的研究应用现状。
6)  Gear Steel 20CrMnTi
20CrMnTi齿轮钢
1.
Effect of MicroaUoyed Ti on Quality of Gear Steel 20CrMnTi;
微合金元素Ti对20CrMnTi齿轮钢质量的影响
补充资料:35CrNi3MoV钢等温淬火组织


35CrNi3MoV钢等温淬火组织


  35CrNi3MoV钢等温淬火组织马氏体(绿)+见氏体(棕)残余奥氏体(浅黄)
  
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条