3) purifying of molten al alloys
铝合金熔体净化
4) Mg-Al alloy melt
镁-铝合金熔体
1.
The results show that electrolyzing SrCl2 and CaCl2 in Mg-Al alloy melt could generate Mg-Al-Sr-Ca alloy directly.
结果表明:在镁-铝合金熔体中电解SrCl2+CaCl2可直接制备出镁-铝-锶-钙合金;当SrCl2与CaCl2物质的量比为1∶1时,熔盐具有良好的可电解性能,其适宜的电解温度为750℃,电解电压为4 V;制备的Mg-6Al-0。
5) Al-Si Alloy
铝硅合金
1.
Modification mechanism of eutectic silicon in Al-Si alloys:impurity-induced coupled twinning;
铝硅合金中共晶硅的变质机理:杂质诱发共生成对孪晶
2.
Mechanism of Acid Pickling for Al-Si Alloy before Spiral Vibration Polishing;
铝硅合金螺旋振动抛光酸洗机理的探讨
3.
Effects of strong magnetic field on modification of Al-Si alloy;
强磁场对铝硅合金变质效果的影响
6) aluminum-silicon alloy
铝硅合金
1.
The effect of heat treatment on the structure and the mechanical property of the aluminum-silicon alloy without solidification shrinkage;
热处理对无凝固收缩铝硅合金组织和性能的影响
2.
Analysis on structure and fracture morphology of short fiber reinforced aluminum-silicon alloy composites;
短纤维增强铝硅合金复合材料的组织与断口形貌分析
3.
Determination of Si,Fe,Zn,Cu,Mn,Ti and Mg elements in aluminum-silicon alloy.;
铝硅合金中硅、铁、锌、铜、锰、钛、镁等元素的同时测定
补充资料:铝-硅系铸造铝合金
分子式:
CAS号:
性质:以硅为主要合金元素的铸造铝合金。硅的添加量范围为5%~25%,并添加镁、铜等元素,形成亚共晶型、共晶型或过共晶型合金。含硅量为5%~13%的亚共晶型或共晶型合金是工业生产中应用最广泛的铸造铝合金。良好的铸造工艺性能和气密性是它们的主要特点。含硅量在13%以上的过共晶型合金具有热膨胀系数小、耐磨性好等特点。
CAS号:
性质:以硅为主要合金元素的铸造铝合金。硅的添加量范围为5%~25%,并添加镁、铜等元素,形成亚共晶型、共晶型或过共晶型合金。含硅量为5%~13%的亚共晶型或共晶型合金是工业生产中应用最广泛的铸造铝合金。良好的铸造工艺性能和气密性是它们的主要特点。含硅量在13%以上的过共晶型合金具有热膨胀系数小、耐磨性好等特点。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条