1) pre-reduced sinter
预还原烧结矿
1.
In this article,the mineral composition and microstructure of pre-reduced sinter from Hainan iron ore under different technical conditions are studied,including forming mechanism of mineral composition and their influence on the characteristics of pre- reduced sinter.
研究了不同工艺条件下海南矿粉预还原烧结矿的矿物组成、含量和显微结构,阐明了预还原烧结矿的形成机理,及矿物组成对其性能的影响。
2) high reducibility sinter
高还原性烧结矿
3) reductive sintering
还原烧结
1.
On the basis of domestic and international literatures on comprehensive extraction of Al and Fe,"reductive sintering-leaching-magnetic separation" process was developed for comprehensively extracting Al and Fe,and studied in detail.
在查阅了大量的国内外综合提取铝铁资料的基础上,选取“还原烧结-溶出-磁选”工艺作为综合提取铁铝的方案,并对此进行了细致地研究。
4) DRI
预还原矿
1.
Influence of Melting Behavior of DRI on Smelting in Melting Gasifier;
预还原矿熔化行为对熔融气化炉冶炼的影响
5) prereduction of iron ore
矿石预还原
6) iron ore prereduction
铁矿石预还原
补充资料:聚四氟乙烯预烧结树脂
分子式:
CAS号:
性质:由悬浮聚四氟乙烯树脂经加压、高温烧结和粉碎等处理而得到的白色颗粒状的聚四氟乙烯树脂。具有聚四氟乙烯的各种优异性能。因系通过预烧结处理,故具有良好的流动性,表观密度大[(600±100)g/L],适用于挤出压力高(一般10~20MPa)的柱塞挤出成型。用预烧结树脂可制得直径5~40mm的棒材和壁厚3~25mm的管材。
CAS号:
性质:由悬浮聚四氟乙烯树脂经加压、高温烧结和粉碎等处理而得到的白色颗粒状的聚四氟乙烯树脂。具有聚四氟乙烯的各种优异性能。因系通过预烧结处理,故具有良好的流动性,表观密度大[(600±100)g/L],适用于挤出压力高(一般10~20MPa)的柱塞挤出成型。用预烧结树脂可制得直径5~40mm的棒材和壁厚3~25mm的管材。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。