1) In situ oxidation/lithiation
原位氧化/锂化
2) atomic lithium oxide
原子能用氧化锂
3) in situ oxidation
原位氧化
1.
Preparation of p-type ZnO thin films by in situ oxidation of Zn_3N_2;
原位氧化Zn_3N_2制备p型ZnO薄膜的性能研究
2.
Smooth ZnO thin films have been obtained by in situ oxidation of Zinc films on mica surfaces.
在云母基底上热蒸镀锌膜,再采用简单的原位氧化方法制备氧化锌薄膜。
4) lithium hydroxide
氢氧化锂
1.
Preparation of lithium hydroxide from lithium sulphate in a three-compartments membrane electrolysis system;
三室膜电解法由硫酸锂制备氢氧化锂的实验研究
2.
A Study on the Regeneration and Utilization of Lithium Hydroxide Used as Gas Purificant;
空气净化用氢氧化锂的再生利用研究
3.
The regeneration of lithium hydroxide used in isolated system has been studied.
氢氧化锂在特殊环境中用作空气净化剂,吸收人体呼吸排出的二氧化碳。
5) lithium peroxide
过氧化锂
6) lithia
[英]['liθiə] [美]['lɪθɪə]
氧化锂
1.
The influences of lithia content on the melting temperature,mechanical properties and thermal expansion coefficient of low temperature frit were studied.
本文研究了氧化锂加入量对低温熔块的熔融温度、力学性能、热膨胀系数的影响。
2.
The silicothermic reaction of lithia in vacuum is analyzed from thermodynamics,and its minimum temperature and the corresponding dew point temperature under different conditions are calculated.
对真空条件下硅热还原氧化锂反应进行热力学分析,计算出不同条件下硅热还原氧化锂所需要的最低反应温度以及相应的露点温度。
补充资料:氧化锂-氧化锌-氧化钒系湿敏材料
分子式:Li2O-ZnO-V2O5
CAS号:
性质:锂锌钒氧化物组成的感湿体材料。感湿过程中,水分子的作用主要是表面附着,使表面电阻下降。具有快的响应速度(吸湿-脱湿时间3~4min),湿滞现象比较轻微,湿阻变化幅度较小,准确性高(<2%RH),重现性好,工作寿命长,测湿范围20%~98%RH。用于制作低温烧结型湿敏电阻。采用800~900℃温度下烧结法制取。
CAS号:
性质:锂锌钒氧化物组成的感湿体材料。感湿过程中,水分子的作用主要是表面附着,使表面电阻下降。具有快的响应速度(吸湿-脱湿时间3~4min),湿滞现象比较轻微,湿阻变化幅度较小,准确性高(<2%RH),重现性好,工作寿命长,测湿范围20%~98%RH。用于制作低温烧结型湿敏电阻。采用800~900℃温度下烧结法制取。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。