说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 裂纹形态发展曲线
1)  crack aspect development curve
裂纹形态发展曲线
1.
Then, some examples of crack aspect development curve (CADC) diagrams were calculated through the present procedure for some typical cracked welded joints subjected to some service loading and residual stress conditions.
以作者建立的焊趾半椭圆表面裂纹应力强度因子数据库以及复杂应力场中焊趾半椭圆表面裂纹前缘应力强度因子分布计算的基本模式法为基础,给出了复杂应力场中焊趾表面裂纹在疲劳扩展过程中形态变化规律及寿命的工程分析方法;并用这个方法计算了一些典型焊接接头在一些典型的外加应力场和残余应力场中的裂纹形态发展曲线
2)  crack growth rate curve
裂纹扩展率曲线
1.
One is the cumulative fatigue damage(CFD) theory based mainly on S-N (or ε-N) curves and the other is the fatigue crack propagation (FCP) theory based on the crack growth rate curve.
一种是基于S-N曲线的累积疲劳损伤理论 ,另一种是基于裂纹扩展率曲线的疲劳裂纹扩展理论。
3)  crack growth curve
裂纹扩展曲线
1.
A method for quickly determining the crack growth curve of offshore steel platforms is presented in the paper.
提出了一种确定海洋平台钢裂纹扩展曲线的快速方法 ,该方法可以综合利用以往的经验数据和当前试验数据确定表面疲劳裂纹扩展速率曲线。
2.
Modeling of crack growth curve is the premise of the durability analysis based on probabilistic fracture mechanism.
裂纹扩展曲线的建模是基于概率断裂力学的耐久性分析方法的前提。
4)  crack developing
裂纹发展
1.
According to observation and analysis rock blasting high-speed photography experiment for deferent solid medium, the basic law of erack developing, and crack length and crack developing speed have been revealed under the deferent blasting methods.
本文通过对不同材质爆破高速摄影试验的观察和分析 ,揭示了在不同爆破方法下裂纹发展的基本规律以及裂纹长度和扩展速度。
5)  curvilinear cracks
曲线裂纹
1.
The torsion fracture problem of bars with curvilinear cracks is investigated.
研究了带曲线裂纹柱体的扭转断裂问题,推导出了可以直接应用于任意形状截面含有任意形状曲线裂纹的柱体扭转问题的新的边界积分方程,并建立了带裂纹柱体扭转问题的边界元数值计算方法,提出了裂纹尖端的奇异元和线性元插值模型,给出了抗扭刚度和应力强度因子的边界元计算公式。
2.
The Saint-Venant torsion problems of a composite cylinder with curvilinear cracks were in- vestigated.
研究含任意曲线裂纹的复合圆柱体的Saint-Venant扭转,将内外材料的交界面视为一边界,将问题划归为内、外边界和裂纹上的积分方程的求解。
3.
There have been many studies about the torsion problem of an isotropic bar with cracks, but most of them are available only to the special section geometry with special curvilinear cracks.
国内外已有不少对于各向同性材料带裂纹柱体扭转的研究,但是仅限于特定截面几何形状和特殊曲线裂纹的问题。
6)  curvilinear crack
曲线裂纹
1.
The Saint-Venant torsion problems of a cylinder with curvilinear cracks were considered and reduced to solving the boundary integral equations only on cracks.
研究含曲线裂纹圆柱的Saint_Venant扭转,将问题化归为裂纹上边界积分方程的求解。
2.
The analytic solution and the intensity factor of anti plane strain problems of curvilinear cracks in piezoelectric materials are obtained by using the Faber series expansion of complex variable functions and solving Hilbert problem.
用复函数的Faber级数展开方法 ,通过求解Hilbert问题研究了含任意曲线裂纹的压电材料反平面应变问题 ,获得了问题的解析解和场强度因子。
补充资料:淬火裂纹和非淬火裂纹的特征及实例分析

淬火裂纹是指在淬火过程中或在淬火后的室温放置过程中产生的裂纹。后者又叫时效裂纹。造成淬火开裂的原因很多,在分析淬火裂纹时,应根据裂纹特征加以区分。


一、淬火裂纹的特征


在淬火过程中,当淬火产生的巨大应力大于材料本身的强度时,便会导致裂纹产生。淬火裂纹往往是在马氏体转变开始进行后不久产生的,裂纹的分布则没有一定的规律,但一般容易在工件的棱角槽口、截面突变处形成。


在显微镜下观察到的淬火开裂,可能是沿晶开裂,也可能是穿晶开裂;有的呈放射状,也有的呈单独线条状或呈网状。


因在马氏体转变区的冷却过快而引起的淬火裂纹,往往是穿晶分布,而且裂纹较直,周围没有分枝的小裂纹。


因淬火加热温度过高而引起的淬火裂纹,都是沿晶分布,裂纹尾端尖细,并呈现过热特征:结构钢中可观察到粗针状马氏体;工具钢中可观察到共晶或角状碳化物。


表面脱碳的高碳钢工件,淬火后容易形成网状裂纹。这是因为,表面脱碳层在淬火冷却时的体积胀大比未脱碳的心部小,表面材料受心部膨胀的作用而被拉裂呈网状。


二、非淬火裂纹的特征


淬火后发生的裂纹,不一定都是淬火所造成的,一般可根据下面的特征来区分。


淬火后发现的裂纹,如果裂纹两侧有氧化脱碳现象,则可以肯定裂纹在淬火之前就已经存在。淬火冷却过程中,只有当马氏体转变量达到一定数量时,裂纹才有可能形成。与此相对应的温度,大约在250℃以下。在这样的低温下,即使产生了裂纹,裂纹两侧也不会发生脱碳和出现明显氧化。所以,有氧化脱碳现象的裂纹是非淬火裂纹。


如果裂纹在淬火前已经存在,又不与表面相通,这样的内部裂纹虽不会产生氧化脱碳,但裂纹的线条显得柔软,尾端圆秃,也容易与淬火裂纹的线条刚健有力,尾端尖细的特征区别开来。


三、实例分析


实例一:


40Cr钢制成的转子轴,经锻造、淬火后发现裂纹。裂纹两侧有氧化迹象,经金相检验,裂纹两侧存在脱碳层,而且裂纹两侧的铁素体呈较大的柱状晶粒,其晶界与裂纹大致垂直。结论:裂纹是在锻造时形成的非淬火裂纹。


当工件在锻造过程中形成裂纹时,淬火加热即引起裂纹两侧氧化脱碳。随着脱碳过程的进行,裂纹两侧的碳含量降低,铁索体晶粒开始生核。当沿裂纹两侧生核的铁素体晶粒长大到彼此接触后,便向离裂纹两侧较远的基体方向生长。由于裂纹两侧在脱碳过程中碳浓度的下降,也是由裂纹的开口部位向内部发展,因而为铁素体晶粒的不断长大提供了条件,故最终长大为晶界与裂纹相垂直的柱状晶体。