1) Progressive forming
逐次成形
2) sequential
逐次
1.
The relations of sensitivity among state variables, measured and estimated values of voltage and power are analyzed, and then a sequential tracking stated estimation method based on sensitivity analysis is proposed.
对状态量、量测量以及功率估计量之间的灵敏度关系进行了分析,进而提出了基于灵敏度分析的逐次追踪状态估计。
3) stepwise regression
逐次回归
1.
In this paper, based on the uniform design principle, an abrasive wear test of Ti-Al coating produced by supersonic arc spraying was conducted, and a stepwise regression analysis was made.
基于均匀设计试验设计方法,进行了超音速电弧喷涂Ti-Al 涂层磨粒磨损试验,在对试验结果进行逐次回归分析的基础上,系统并定量的研究了涂层耐磨性能随着喷涂工艺参数的变化规律,得到了优化后的最佳喷涂工艺参数。
4) gradual approach
逐次逼近
1.
In order to eliminate systemic error caused by different times, different labs, different analysis methods, and to solve some problems in merging maps, we propose a map adjustment theory and gradual approach method, based on a hypothesis that there are same means and standard deviate of data in adjacent small areas between maps.
针对区域地球化学中因不同时间、不同实验室、不同分析手段等原因存在于各图幅数据的系统偏差而造成的图边拼接问题,提出了抑制图幅间数据系统误差影响的图幅平差思想,阐述了图幅平差的数学原理及逐次逼近平差方法。
2.
By means of constructional iterative equationthis paper presents a way to give out the existence and singularity of a type of e- quational root with gradual approach method.
本文通过构造迭代函数,利用逐次逼近的方法给出了一类方程根的存在性与唯一性的判断的一种解决方案。
3.
Kepler s equations can be solved with the gradual approach, which can be further extended to the solution of the non-linear equations.
求解开普勒方程可用逐次逼近法 ,这种方法还可推广到非线性方程的求解问题中。
5) sequential tracing
逐次追踪
6) successive approximation
逐次逼近
1.
Capacitor self-calibration technique used in time-interleaved successive approximation ADC;
时间交叉存取逐次逼近型ADC中的电容自校准技术(英文)
2.
SDP with successive approximation and its application in the operation of multireservoir system;
逐次逼近随机动态规划及库群优化调度
3.
According to IEEE standard for short time disturbance of power quality,a fast successive approximation classification method is developed.
针对电力短时扰动信号具有非平稳、突发性的特点,应用小波变换的多分辨率分析特性检测扰动信号的特征参量,依据IEEE制定的短时电能质量扰动标准,提出了一种逐次逼近型的快速分类法。
参考词条
补充资料:主要射出成形材料成形时应注意事项
■主要射出成形材料成形时应注意事项
品 名 注 意 事 项
PVC
聚氯乙烯
1. 产品种类范围非常广(硬质、软质、聚合物等),成型条件各有不同,从熔融至分
解之温度范围很小,尤须注意加热温度。
2. 附着水分少,但成型周期尽可能减少(50℃~60℃热风干燥)。
3. 成型机方面,与材料直接接触的部位须电镀或采用不锈钢以防热分解所产生的盐酸
侵蚀。射出压力2100kg/cm2程度。
4. 所有塑料当中必须是细心注意温度调节。
5. 浇口附近易产生流纹,故射出操作后,柱塞不要后退使浇口充分固化后再瞬间退后为宜。
6. 加热之初温不宜高,特别注意熔融情形。第二级加热温度较高,且尽可能使成形周
期缩短,比较安全。
PA
聚醯胺树脂
1. 成型温度比其它材料高,故采用油加热的成形机较适当。
2. 吸湿性大,必须充分干燥。水分对成型品的品质影响甚大(80℃热风干燥约5~6小时)。
3. 须退火以消除内部歪斜。
PP
聚丙烯
1. 同PE,但成形温度必须较高。熔融温度170℃,超过190℃则流动性大增,则毛边增加,
易产生接缝及凹入情形。
PC
聚碳酸脂
1. 吸湿性比尼龙小,但若有些微之水分存在则成型品产生其它色泽或气泡,故必须密封
干燥同时成形时也须预备干燥(120℃之温度4小时)。
2. 加热温度超过320℃时则产生热分解,成品变色,故特别注意温度调节,又成型时的温度调节也非常重要,须特别注意其最低温度、最低时间。
3. 须退火以消除内部歪斜(130℃~135℃,1小时程度为准)。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。