1) long glass fiber reinforced polypropylene
长玻璃纤维增强聚丙烯
1.
Using an impregnation and pultrusion device developed at our laboratory, long glass fiber reinforced polypropylene pellets for injection molding were produced.
利用自行研制的连续纤维 /热塑性树脂浸渍装置 ,制备了注塑成型用长玻璃纤维增强聚丙烯粒料。
2) glass fiber reinforced polypropylene
玻璃纤维增强聚丙烯
1.
To reduce the warpage of glass fiber reinforced polypropylene(PP/GF) products,the effects of five injection molding parameters including mold temperature,nozzle temperature,injection speed,hold pressure and hold time on the mold shrinkage and the warpage of PP/GF products were investigated.
针对玻璃纤维增强聚丙烯(PP/GF)注射成型制品存在的翘曲变形缺陷,研究了注射工艺参数如模具温度、喷嘴温度、注射速率、保压压力和保压时间对制品成型收缩率及翘曲的影响。
2.
Therefore, the shrinkage of the glass fiber reinforced polypropylene specimens prepared by injection was investigated with the combination of the experiments and the simulation.
本工作采用试验与数值模拟相结合的研究方法,对玻璃纤维增强聚丙烯系列材料的成型收缩率进行了深入研究。
3) Acrylafil
艾克里拉菲尔[中长玻璃纤维增强聚丙烯酸酯][商]
4) fiber glass reinforced polypropylene partition valve
玻璃纤维增强聚丙烯隔膜阀
5) Glass fiber reinforced PP pipe
玻璃纤维增强聚丙烯管材
6) Profil
普罗菲尔(玻璃纤维增强聚丙烯)<商>
补充资料:聚丙烯
聚丙烯 polypropylene 丙烯的聚合物。英文缩写PP。结构为 熔融温度约174℃,密度0.91克/厘米3。强度高,硬度大,耐磨,耐弯曲疲劳,耐热达 120℃,耐湿和耐化学性均佳,容易加工成型,价格低廉 ,因此是产量大(1990年世界年产量已逾500万吨 )、应用广泛的通用高分子品种。缺点是低温韧性差,不耐老化。近年来通过共聚和共混等方法改进。 单体丙烯由石油裂解或炼油尾气分离提纯得到 ,纯度应在99.5%以上 ,少量杂质能使催化剂中毒。聚合方法有淤浆、液相本体和气相聚合3 种,以后二者为主。催化剂常为齐格勒纳塔型,如δ-TiCl3-(C2H5)2AlCl或TiCl3-(C2H5)Al,效率300~900克聚丙烯/克TiCl3。近年则用MgCl2作载体并添加苯甲酸酯的钛-铝体系 ,效率高达70~100千克聚丙烯/克钛,并免后处理工艺。
聚丙烯可用注射、挤出、吹塑、层压、熔纺等工艺成型,也适于双向拉伸。广泛用于制造容器、管道、包装材料、薄膜和纤维,也常用增强方法获得性能优良的工程塑料。大量应用于汽车、建筑、化工、医疗器具、农业和家庭用品方面。聚丙烯纤维的中国商品名为丙纶。强度与耐纶相仿而价格低廉,用于织造地毯、滤布、缆绳、编织袋等。 |
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条