1) Rotary rolling caused flaw
斜轧缺陷
2) Roll defect
轧辊缺陷
1.
Firstly,advanced inspection methods such as magnaflux method,portable roll surface rigidity detector,macrostructure analysis and so on should be applied to find out the roll defects,which are difficult to be observed with naked eyes.
以1200HC6辊可逆冷轧机轧辊为研究对象,从轧辊检测、磨削和装配等多方面提出了轧辊缺陷的预防和消除措施。
3) rolled defect
轧制缺陷
1.
Influence of rolled defects on performance of hot upset forging of round steel were discussed.
以莱芜钢铁股份有限公司电炉连铸坯和圆钢为研究对象,探讨了轧制缺陷对圆钢热顶锻性能的影响,并对常见轧制缺陷,如折叠、辊印、褶皱,引起热顶锻开裂的原因、形态特征进行了分析比较,从而可及时准确地进行裂纹辩识,并指导生产。
5) rolling defect
轧制缺陷<冶>
6) roller surface defect
轧辊表面缺陷
1.
Detection of roller surface defect is an important question in the roller profile online measurement system.
轧辊表面缺陷检测是轧辊辊型在线检测系统中的一个重要问题 ,它直接影响着带材产品的质量 ,传统的检测方法和数据分析方法已经很难适应现代的轧制生产。
补充资料:孔型斜轧
孔型斜轧
helical groove skew rolling
kongxing xiezha孔型斜轧(helieal groove skew rolling)用带有变高度、变螺距的螺旋孔型并札变断面回转体零件的回转成形工艺。孔型斜轧时,两个或三个轧机的轴线相互交叉成一定角度,并做同向等速旋转,轧辊表面上有螺旋状孔型,轧件在轧辊孔型的作用下边旋转边前进被轧制成所需要形状和尺寸的回转体零件,如图所示。 ;巍缈一3 2目……喊阳乙 孔型斜轧示意图 1一轧辊;2一坯料;3一零件 用孔型斜轧工艺可以生产钢球、铣刀坯等实心件、轴承环、自行车脚闸毛坯等空心件以及丝杠、翅棱管等螺旋面零件等。孔型斜轧回转体零件具有生产率高、产品质量好、无噪音等公害并易于实现机械化自动化等优点。但孔型斜轧的轧辊设计及制造比较复杂。 孔型斜轧自20世纪40~50年代在苏联、日本、美国等国家得到发展和应用以来,工艺日趋成熟,不仅有定型专用设备,而且出现自动生产线。中国从5。年代开始从事孔型斜轧研究工作,并取得了很大进展。 轧件的旋转和运动坯料被咬入轧辊,首先是在咬人锥部被咬入后,坯料受到径向压缩,由此产生的轴向分力使坯料向轧辊孔型段内运动,然后坯料被孔型部分咬人。坯料在孔型中主要靠轧辊凸棱带动旋转并给以压下量而成形。为了保证坯料的咬入和旋转,坯料每转半转内允许的最大压下量Z应满足下式: Z尸 /一打,+姜{ ’、占’D}式中d为坯料直径;f为轧件与轧辊间摩擦系数;泞为坯料椭圆系数;D为轧辊直径。 轧件在螺旋孔型中斜轧时,边旋转边前进,即作螺旋前进运动。轧件之所以能够沿轴向前进,不只是由于轧辊圆周速度沿轧件轴线方向的分量带动轧件运动,还由于轧辊旋转时螺旋孔型对轧件的推动作用。当轧辊摩擦带动轧件向前运动的速度等于轧辊螺旋孔型推动轧件向前运动速度时,轧制平稳,不会发生孔型凸棱切入轧件前后端面现象。由此可得出如下结论:为了实现平稳而无前后孔型凸棱挤压轧件的轧制,在调整时应使轧辊的倾斜角度等于轧辊孔型的螺旋升角。 斜轧孔型特点斜轧孔型具有如下特点: (1)孔型为螺旋形。两螺旋面构成的凸起称为凸棱。相邻凸棱之间的型槽叫做孔型型腔。孔型螺旋长度以度数(a)表示,长度划分以凸棱为基准,通常按900等分,并规定自棒料咬入、成形到精整、切断,按a值递减进行标注。 (2)孔型一般由两部分组成:成形区和精整区,成形区与精整区是连续的。型腔槽底是等高面,即在同一圆周面上。成形区凸棱由低变高,型腔由浅而深,反映了轧件的成形过程。