The principle,factors and the role of various factors of coke formation process of disengager were expounded.
阐述了沉降器内油气结焦的原理,影响因素及各因素的作用,分析了结焦的形成过程,平均停留时间对结焦量的影响以及流动状态对结焦形貌的影响,介绍了防止沉降器结焦的研究进展情况和存在的问题。
2.
The rigidity of coke was chiefly affected by the ways of oil droplets and catalyst particles accumulating and/or depositing together during coke formation.
采用扫描电镜(SEM)和X射线能谱分析仪对催化裂化装置(FCCU)沉降器内结焦物的微观组织结构和成分进行了分析,将结焦物划分为软焦和硬焦。
3.
In ethylene furnaces,coke formation reduces product yields,increases energy consumption and shortens runlength.
综述了近年来国内外乙烯裂解过程中结焦抑制技术研究及工业应用进展 ;介绍了添加结焦抑制剂、炉管涂覆技术研究、新材料炉管的工业应用 ;对中国乙烯装置开发结焦抑制技术提出了建
3) coking
结焦
1.
Steel HP40 Coated by Alumina Film and Its Anticoking Ability;
HP40钢表面沉积Al_2O_3薄膜及其抗结焦性能
2.
Analysis of coking mechanisms in residue fluid catalytic cracking disengagers;
重油催化裂化沉降器结焦历程分析
3.
Analysis and method to slow down the coking of the big gas-oil line in delayed coking system;
延迟焦化大瓦斯线结焦分析及减缓措施
4) coke
结焦
1.
Studies on Mechanism of Coke by the Pyrolysis of Hydrocarbon;
烃类裂解结焦机理的研究
2.
Anti-Coking Performance of a New Coke Inhibitor FPA-151;
新型结焦抑制剂FPA-151抑焦性能的研究
3.
Development of Hydrocarbon Pyrolysis Coke Inhibitor Technology (Ⅰ);
烃类蒸汽裂解结焦抑制剂技术进展(上)
5) agglomeration
结焦
1.
The Reason and Prevention of Biomass Agglomeration in a Fluidized Bed Gasifier;
生物质流化床气化结焦的原因与预防
2.
Agglomeration and defluidization behaviors often occur in the high fluidized bed, studies for agglomeration in fluidized beds are summarized in this paper.
分析了近年来高温流化床结焦研究的状况,总结了流化床结焦现象及其影响因素、流化床结焦时的最小流化速度及影响因素、流化床结焦机理, 并分析了研究中存在的问题, 探讨了高温流化床结焦特性研究的方向。
3.
were analyzed from structure,coal quality and combustion adjustment,and the agglomeration preventing methods were raised.
从锅炉结构、煤质、燃烧调整方面对攀钢发电厂锅炉结焦原因进行了分析,提出了防止锅炉结焦的办法。
6) slagging
结焦
1.
Analysis and Preventive of the Circulating Fluidized Bed Boiler Slagging;
流化床锅炉结焦原因的分析及预防
2.
Analysis of the FI CIRC~(TM) Fluidized Bed Boiler Slagging in Waste Heat Power Station in Cement Plant;
某水泥厂余热电站FI CIRC~(TM)循环流化床锅炉结焦原因的分析
3.
Cause analysis of serious slagging in Unit 4 boiler of Shaoguan Power Plant and countermeasures;
韶关发电厂4号炉结焦严重的原因分析及对策
参考词条
补充资料:催化结焦
分子式:
CAS号:
性质:指发生在催化剂(金属,金属氧化物或硫化物)表面上,主要通过硅铝酸催化剂在高温下与烃接触催化聚合反应(催化裂解的副反应),生成结焦产物的过程。
CAS号:
性质:指发生在催化剂(金属,金属氧化物或硫化物)表面上,主要通过硅铝酸催化剂在高温下与烃接触催化聚合反应(催化裂解的副反应),生成结焦产物的过程。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。