您的位置:首页 -> 词典 -> 金属基陶瓷涂料
1)  metallic matrix ceramic coating
金属基陶瓷涂料
2)  metal-ceramic paint
金属陶瓷涂料
1.
Performance and application in anti-corrosion area of metal-ceramic paint are given.
介绍了金属陶瓷涂料的性能及在防腐蚀方面的应用。
3)  ceramic coating/metal substrate
金属基/陶瓷涂层
4)  ceramal composite coating
金属陶瓷复合材料涂层
1.
Wear properties of reactive plasma clad (Cr,Fe)_7C_3/γ-Fe ceramal composite coatings;
反应等离子熔覆(Cr,Fe)_7C_3/γ-Fe金属陶瓷复合材料涂层的耐磨性
2.
A new type in-situ reinforcing Cr_7C_3 ceramal composite coating was fabricated on carbon steel(C_3) substrate by plasma cladding.
采用等离子熔覆技术,在调质C3钢表面制得以原位生成初生相Cr7C3为增强相的金属陶瓷复合材料涂层;利用SEM、XRD和EDS等分析了涂层的显微组织和相组成;测试了在室温干滑动磨擦及高温滑动磨擦条件下涂层的耐磨性,并讨论了其磨损机理。
5)  Ni-based metal-ceramics layers
镍基金属陶瓷涂层
6)  Cr3C2 matrix cermet coating
Cr3C2基金属陶瓷涂层
1.
The Cr3C2 matrix cermet coatings with BaF2/CaF2 eutectic addition were made by detonation gun spraying.
采用爆炸喷涂制备添加BaF2/CaF2共晶的Cr3C2基金属陶瓷涂层,通过X射线衍射仪(XRD)、扫描电镜(SEM)及显微硬度仪等检测方法观测了喷涂粉形貌、相组成及涂层微观组织、硬度等性能,探讨了BaF2/CaF2共晶的加入方式及其含量对爆炸喷涂Cr3C2基金属陶瓷涂层性能的影响,结果显示:10%的BaF2/CaF2共晶与Cr3C2-25%NiCr粉体经高能球磨1h,粉体粒度最小,尺寸均匀性最高。
补充资料:活性金属法陶瓷-金属封接
分子式:
CAS号:

性质:将活性金属粉(如钛、锆、铪等)与,有机溶剂调合成膏状涂敷在要封接的陶瓷表面上。在涂有活性金属粉的陶瓷和金属零件之间放置能在较低温度下形成合金的金属焊料(如银、铜、镍、银-铜等),在真空或惰性气氛中加热而使陶瓷-金属气密性封接的一种方法。活性金属对各种氧化物和硅酸盐均有较强的亲和力,可实现气密封接。以钛;银-铜法用得最为广泛。活性封接法的优点是工序少、周期短、瓷件不会变形,成品率高。但结构上对针封、套封较困难,也很难连续生产。 