The new developing ideal of preparing advanced cemented carbide tool material with excellent performance by means of whisker reinforcing and nano crystalline compounding technologies is presented.
回顾了常规刀具材料的基本性能 ,从细化晶粒、表面涂层、热处理、添加稀有金属和稀土元素等方面综述了硬质合金刀具材料的研究现状 ,提出采用晶须增韧补强、纳米复合强化技术制备新型高性能硬质合金刀具材料的发展思
2.
The interaction of whisker reninforcing and phase transformation toughening in the matrix when combining this two toughening techniques is analyzed on the basis of reviewing the mechanisms of whisker reinforcing and phase transformation toughening and the effects of oxide ceramics toughened by thecombined toughening technique in the civil and abroad are summarized in this paper.
在综述陶资材料晶须增韧和相变增韧机制的基础上,分析了晶须增韧和相变增韧复合时的相互作用,并介绍了国内外利用复合增韧法韧化氧化物陶瓷的研究结果,同时指出了存在的问题和获得优良复合增韧效果的有效途径。
2)  whisker-reinforced ceramics
晶须增韧陶瓷
1.
The fractal characteristics of JX-1 whisker-reinforced ceramics is studied.
研究JX-1型晶须增韧陶瓷断口的分形特征,测量材料断口表面的分形维数,建立分形维数与断裂韧性间的关系。
3)  sic-cvystall increasingly-malleable ceramics
碳化硅晶须增韧陶瓷
4)  whisker toughening
晶须韧化
5)  whisker reinforcement
晶须增强
6)  silicon carbide whisker reinforced alumina matrix composite
碳化硅晶须增韧氧化铝复合材料
补充资料:多晶莫来石晶须(纤维)
分子式:
CAS号:

性质:莫来石相为主晶相的多晶纤维。化学成分为Al2O3 72%~77%,SiO222%~17%,B2O3 3%~5%,P2O51.5%~3.0%。纤维直径2~7μm,纤维长度20~125μm。使用温度1350℃。多采用溶胶-凝胶法制造。主要用作补强填料,也可作为轻质、隔热保温材料使用。